Method and manufacturing carbon-containing modified polystyrene resin foamed particles, and a method of manufacturing the same carbon-containing modified polystyrene resin foamed article

机译:含碳改性聚苯乙烯树脂发泡颗粒的方法和制造方法,以及制造该含碳改性聚苯乙烯树脂发泡体的方法

摘要

PROBLEM TO BE SOLVED: To provide a carbon-containing modified polystyrene resin foam molded article which has heat resistance and blackness improved more than those of a conventional carbon-containing modified polystyrene resin foam molded article.;SOLUTION: Carbon-containing modified polystyrene resin foam particles are obtained by preliminary foaming, to a bulk foaming multiple of 20-45 times, carbon-containing expandable modified polystyrene resin particles obtained by impregnating a blowing agent into carbon-including modified polystyrene resin particles including 100-400 pts.mass of a polystyrene resin per 100 pts.mass of a carbon-including polypropylene resin. The film thickness of the most superficial layer of the foam particles, calculated from an image observed with a scanning electron microscope, is 5-25 μm. The average bubble diameter of air bubbles contacting to the most superficial layer of the foam particles calculated from an image observed with a scanning electron microscope, is 100-600 μm.;COPYRIGHT: (C)2011,JPO&INPIT
机译:要解决的问题:提供一种含碳改性聚苯乙烯树脂泡沫模塑制品,其耐热性和黑度比常规的含碳改性聚苯乙烯树脂泡沫模塑制品改善得多。通过将发泡剂浸渍到含碳量为100-400 pts的含碳改性聚苯乙烯树脂颗粒中,将含碳的可发泡改性聚苯乙烯树脂颗粒初步发泡至20-45倍的整体发泡倍数来获得。每100点质量的含碳聚丙烯树脂中的树脂。由用扫描电子显微镜观察的图像计算出的泡沫颗粒的最表层的膜厚度为5-25μm。根据用扫描电子显微镜观察到的图像计算出,与泡沫颗粒的最表面层接触的气泡的平均气泡直径为100-600μm。版权所有:(C)2011,JPO&INPIT

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号