Method for manufacturing corrugated flexible tube, apparatus for manufacturing the same, and corrugated flexible tube

机译:波纹状挠性管的制造方法,制造装置以及波纹状挠性管

摘要

PPROBLEM TO BE SOLVED: To provide a manufacturing method of a corrugated flexible pipe improved in flexibility and enhanced in productivity and product quality, despite a fact that a partition wall is provided, a manufacturing apparatus of the corrugated flexible pipe and the corrugated flexible pipe. PSOLUTION: A cylindrical uncured resin 4A for a pipe wall is continuously extruded from the first resin extrusion port 5A of the first die 5 arranged on the upstream side of a molding route part B1 and closely brought into contact with the half peripheral wall molding surfaces 3a and 3b of both split molds 3A and 3B to form the corrugated flexible pipe 1 having a large diameter pipe wall part 1A, a small diameter pipe wall part 1B and the side wall part 1C for connecting them. The resin 4B for the partition wall in an uncured state continuously extruded from the second resin extrusion port 6A formed to a second die 6 is fused or welded to the inner peripheral surface of the small diameter pipe wall part 1B or a region provided over the inner peripheral surface of the small diameter pipe wall part 1B and a part of the inner peripheral surface of the side wall part 1C continued thereto in a state traversing the inside of the corrugated flexible pipe 1 closely brought into contact with the half peripheral wall molding surfaces 3a and 3b and under an uncured state to form the partition wall 2 for demarcating the inside of the pipe. PCOPYRIGHT: (C)2008,JPO&INPIT
机译:

要解决的问题:提供一种波纹挠性管的制造方法,该波纹挠性管尽管设置了分隔壁,但挠性提高,生产率和产品质量提高,该波纹状挠性管的制造装置和波纹挠性管。

解决方案:从设置在成型路径部分B1上游侧的第一模具5的第一树脂挤出口5A连续挤出用于管壁的圆柱形未固化树脂4A,并使其紧密接触半周壁。分开的模具3A和3B的两个模制表面3a和3b形成具有大直径管壁部分1A,小直径管壁部分1B和用于连接它们的侧壁部分1C的波纹状挠性管1。从形成于第二模具6的第二树脂排出口6A连续挤出的未固化状态的隔壁用树脂4B熔接或焊接在小径管壁部1B的内周面或设置于其内部的区域。小直径管壁部1B的周面和侧壁部1C的内周面的一部分以与波纹状挠性管1的内部紧密地横穿且与半周壁成型面3a接触的状态连续。如图3A和3B所示,在未固化状态下形成用于分隔管子内部的分隔壁2。

版权:(C)2008,日本特许厅&INPIT

著录项

  • 公开/公告号JP5103010B2

    专利类型

  • 公开/公告日2012-12-19

    原文格式PDF

  • 申请/专利权人 因幡電機産業株式会社;

    申请/专利号JP20060337105

  • 发明设计人 佐藤 勝;

    申请日2006-12-14

  • 分类号B29C47/12;B29L23/18;

  • 国家 JP

  • 入库时间 2022-08-21 16:55:15

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号