PPROBLEM TO BE SOLVED: To raise productivity, when applying cylindrical deep-drawing to an austenitic stainless steel plate, by decreasing a forming speed just before a punch is brought into contact with the austenitic stainless steel plate to be drawn and increasing the forming speed at the stage where the forming exceeds a crack generation portion. PSOLUTION: When applying cylindrical deep-drawing to the austenitic stainless steel plate 1 to be drawn, which is fixed with a die 3 and a blank holder 4, by pressing a punch 2 into the plate 1, a preliminary deep-drawing, in which drawing is preliminarily conducted to a deep-drawing height where a crack is generated, is carried out. The height from the position, where a crack is generated on the preliminarily drawn product, to the top part of the deep-drawing is measured. When actually conducting the deep-drawing, the forming speed is decreased just before the punch 2 is brought into contact with the austenitic stainless steel plate 1 to be drawn, and increased after the deep-drawing is carried out at least by the height from the position, where a crack is generated on the preliminarily drawn product, to the top part of the deep-drawing. PCOPYRIGHT: (C)2010,JPO&INPIT
机译:

要解决的问题:为了提高生产率,在对奥氏体不锈钢板进行圆柱形深冲时,通过在冲头与要拉伸的奥氏体不锈钢板接触之前降低成形速度,并增加在成形超过裂纹产生部分的阶段的成形速度。

解决方案:当对要拉伸的奥氏体不锈钢板1进行圆柱深冲时,通过用冲头2将冲头2压入板1中,该板由模具3和坯料支架4固定,从而进行初步深冲首先进行拉深至产生裂纹的深冲高度。测量从在初步拉伸的产品上产生裂纹的位置到深冲的顶部的高度。当实际进行深冲时,在将冲头2与要拉伸的奥氏体不锈钢板1接触之前降低成形速度,并且在深冲之后至少从距冲头2的高度提高成形速度。在预拉伸产品上产生裂纹的位置到深拉伸的顶部。

版权:(C)2010,日本特许厅&INPIT

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号