Fluorine-containing copolymer of high molecular weight having a melt viscosity of the melting point + 15 ℃ is 1500~35000Pa · s, and repeating units based on ethylene and repeating units based on tetrafluoroethylene (A), a of the melting point + 15 ℃ melt viscosity of 50~3000Pa · s, melt viscosity at the melting point + 15 ℃ fluorinated copolymer (A) is one-fifth of the melt viscosity at the same temperature fluorine-containing copolymer (A) The less, the fluorine-containing copolymer of low molecular weight having repeating units based on ethylene and repeating units based on tetrafluoroethylene fluorinated copolymers from (A) (B), and fluorine-containing copolymer (A) and a solvent capable of dissolving the fluorine-containing copolymer (A) and (B) at a temperature below the melting point of (B) fluorine-containing copolymer and (A) (B) a mixture comprising a (C) and (D) There is heated to a temperature above dissolving solvent (C), and a solution state, then the process for producing a fluorine-containing copolymer composition to remove the solvent (C).
机译:熔点+ 15℃的熔融粘度的高分子量含氟共聚物为1500〜35000Pa·s,基于乙烯的重复单元和基于四氟乙烯的重复单元(A)的熔点a + 15℃熔体粘度为50〜3000Pa·s,含氟共聚物(A)的熔点+ 15℃时的熔体粘度是相同温度下的熔体粘度的五分之一。具有(A)(B)的基于乙烯的重复单元和基于四氟乙烯的含氟共聚物的重复单元的低分子量,以及含氟共聚物(A)和能够溶解含氟共聚物(A)的溶剂,并且B)在低于(B)含氟共聚物和(A)的熔点的温度下(B)将包含(C)和(D)的混合物加热到高于溶解溶剂(C)的温度,溶液状态,然后是生产过程除去溶剂(C)的含氟共聚物组合物。

著录项

  • 公开/公告号JPWO2011129405A1

    专利类型

  • 公开/公告日2013-07-18

    原文格式PDF

  • 申请/专利权人 旭硝子株式会社;

    申请/专利号JP20120510689

  • 发明设计人 射矢 健;佐藤 崇;

    申请日2011-04-14

  • 分类号C08L27/18;C08J3/20;

  • 国家 JP

  • 入库时间 2022-08-21 16:54:24