In mass%, this soft-nitriding steels, C: 0.15% and less than 0% or more, Si: 0.01~1.00%, Mn: 0.01~1.00%, S: 0.0001 1.50% or less and ultra-0.50%, N:: ~0.050%, Al: 0.0001~0.050%, Ti and containing 0.0005 to 0.0100%, the balance being Fe and inevitable consists impurities, P: 0.050% or less, O: and and limited to 0.0060% or less Ti content and [Ti%], C and the amount of [C%], N and the amount of [N%], S amount and [S%] but, 0.48 [Ti%] - to satisfy the ≦ 1.20 ([S%] / 32 [N%] / 14+ [C%] / 12+) 47.9 ×.
机译:以质量%计,该软氮化钢C:0.15%且小于0%; Si:0.01〜1.00%; Mn:0.01〜1.00%; S:0.0001 1.50%以下;超0.50%; N ::〜0.050%,Al:0.0001〜0.050%,Ti,含有0.0005〜0.0100%,余量为Fe,不可避免地包含杂质,P:0.050%以下,O:且为0.0060%以下。 [Ti%],C和[C%]的量,N和[N%]的量,S和[S%],但0.48 <[Ti%]-满足≤1.20([S% ] / 32 [N%] / 14+ [C%] / 12+)47.9×。

著录项

  • 公开/公告号JPWO2011114775A1

    专利类型

  • 公开/公告日2013-06-27

    原文格式PDF

  • 申请/专利权人 新日鐵住金株式会社;

    申请/专利号JP20110525054

  • 发明设计人 久保田 学;

    申请日2011-01-25

  • 分类号C22C38/00;C22C38/60;C21D1/06;C21D9/32;C21D9/28;C21D9/40;C23C8/26;

  • 国家 JP

  • 入库时间 2022-08-21 16:54:15

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号