PROBLEM TO BE SOLVED: To provide a low yield ratio steel for low temperature use which is excellent in low-temperature toughness, and is suitable as the steel for a multi-purpose tank.;SOLUTION: The steel for low temperature use contains C, Si, Mn, P, S, Nb, Ti, sol.Al, N, contains two or more elements of Cu, Ni, Cr, Mo and the balance Fe with inevitable impurities, and satisfies the following formula, SP1=Cr/5+Mo/3+(Cu+Ni)/15 is 0.06-0.12%. At the position of t/4 where (t) is the thickness of the steel sheet, the texture is diplophase texture of ferrite structure and hard texture structure. The hardened structure satisfies the following formula Hvh/Hvm≥3.0, and contains ≥15 pieces in the range of 100 μm square, and the average grain diameter corresponding to the circle average grain diameter corresponding to the circle of the hardened structure is 2-5 μm. The same of the ferrite structure is 7.5-20 μm, and the aspect ratio thereof is ≤2.0. Wherein, the Hvh and the Hvm express the Vickers hardness of the hardened structure and the perrite structure respectively.;COPYRIGHT: (C)2010,JPO&INPIT
机译:要解决的问题:提供一种低温屈服比低的钢,该钢具有优异的低温韧性,并适合用作多用途罐的钢。;解决方案:低温钢含有C, Si,Mn,P,S,Nb,Ti,sol.Al,N包含Cu,Ni,Cr,Mo和余下的Fe中的两种以上元素,且不可避免地存在杂质,并满足下式SP1 = Cr / 5 + Mo / 3 +(Cu + Ni)/ 15为0.06-0.12%。在t / 4的位置,其中(t)是钢板的厚度,织构是铁素体组织和硬织构的双相织构。硬化结构满足下式Hvh /Hvm≥3.0,并且包含在100μm见方范围内的≥15个,并且与对应于硬化结构的圆的圆形平均粒径相对应的平均粒径为2-5微米铁素体结构的相同点为7.5〜20μm,长径比为2.0。其中,Hvh和Hvm分别表示硬化组织和珍珠岩组织的维氏硬度。;版权所有:(C)2010,JPO&INPIT

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号