Disclosed is a method for preparing intelligent stress response type silicon-boron polymer micro-gel, comprising the following steps of: performing agitation reaction on pre-polyreaction liquid under 70-130°C for 1-6 hours; adding a di-functional chain extender to continue the agitation reaction for 2-6 hours with a reaction temperature being 30-90°C; and finally adding a functional modifying agent to perform the agitation reaction under 30-120°C for 4-8 hours, so as to obtain the intelligent stress response type silicon-boron polymer micro-gel. The pre-polyreaction liquid comprises: low molecular weight polyorganosiloxane occupying 75.0-96.5% of the mass of the pre-polyreaction liquid by weight; and a boron containing compound occupying 3.50-25.0% of the mass of the pre-polyreaction liquid by weight. The method for preparing intelligent stress response type silicon-boron polymer micro-gel of the present invention has a low reaction temperature and a simple operation, does not need a catalyser to be introduced, and facilitates large-scale production.
机译:本发明公开了一种智能应力响应型硅-硼聚合物微凝胶的制备方法,包括以下步骤:在70-130℃下对预聚反应液进行搅拌反应1-6小时;加入双官能扩链剂,使反应温度为30-90℃,继续搅拌2-6小时。最后加入功能性改性剂,在30-120℃下搅拌4-8小时,得到智能应力响应型硅硼聚合物微凝胶。所述预聚反应液包含:低分子量聚有机硅氧烷,其占所述预聚反应液的质量的75.0-69.5重量%。含硼化合物占预聚反应前液体重量的3.50-25.0%。本发明的智能应力响应型硅硼聚合物微凝胶的制备方法反应温度低,操作简单,不需要引入催化剂,便于大规模生产。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号