PURPOSE: A polysilsesquioxane microfiber of a ladder type using electrospinning and a method for fabricating the same are provided to ensure excellent thermal resistance and chemical resistance. CONSTITUTION: A polysilsequioxane microfiber of a ladder type contains polysilsesquioxane of chemical formula 1. In chemical formula 1, R is selected from the group consisting of organic functional groups. The polysilsesquioxane is denoted by chemical formula 2 or 3. The thickness of the microfiber is 1-10 um. A method for fabricating the microfiber comprises a step of electrospinning a solution containing polysilsesquioxane and a step of irradiating UV ray. A solvent used in the solution is tetrahydrofurane, dimethyl formamide, dimehtyl acetamide, N-methyl-2-pyrrolidone, hexane, cyclohexane, toluene, xylene, cresol, chloroform, dimethyl benzene, trimethyl benzene, pyridine, methyl naphthalene, nitromethane, acrnitrile, methylene chloride, aniline, dimethyl sulfoxide, or benzyl alcohol.
机译:目的:提供使用静电纺丝的梯型聚倍半硅氧烷微纤维及其制造方法,以确保优异的耐热性和耐化学性。组成:梯型聚倍半硅氧烷微纤维包含化学式1的聚倍半硅氧烷。在化学式1中,R选自有机官能团。聚倍半硅氧烷由化学式2或3表示。超细纤维的厚度为1-10μm。一种制造超细纤维的方法,包括静电纺丝包含聚倍半硅氧烷的溶液的步骤和照射紫外线的步骤。溶液中使用的溶剂是四氢呋喃,二甲基甲酰胺,二甲基乙酰胺,N-甲基-2-吡咯烷酮,己烷,环己烷,甲苯,二甲苯,甲酚,氯仿,二甲基苯,三甲基苯,吡啶,甲基萘,硝基甲烷,腈,二氯甲烷,苯胺,二甲基亚砜或苯甲醇。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号