PURPOSE: A palladium-alumina complex catalyst for manufacturing gamma-butyrolactone based on the hydrogenation of succinic acid, a method for manufacturing the same, a method for manufacturing the gamma-butyrolactone using the catalyst are provided to use waste succinic acid as environmentally-friendly materials replacing maleic anhydride. CONSTITUTION: A palladium-alumina complex catalyst for manufacturing gamma-butyrolactone based on the hydrogenation of succinic acid includes an Al-O-Pd structure based on the chemical bond of alumina and palladium. In the complex catalyst, the content of palladium is 1 to 10 weight% of the total weight of alumina. The average pore size of the complex catalyst is between 2nm and 10nm. The surface area of the complex catalyst is between 10m^2/g and 400m^2/g. A method for manufacturing the complex catalyst includes the following: An aluminum precursor is dissolved, water and hydration synthetic catalyst are added to form alumina sol; a palladium precursor alcohol solution is added into the alumina sol to synthesize alumina-palladium complex sol; the alumina-palladium complex sol is cooled, and water is added into the cooled complex sol to obtain palladium-alumina complex gel; and the complex gel is aged, dried, and plasticized.
机译:目的:提供一种基于琥珀酸加氢制造γ-丁内酯的钯-氧化铝复合催化剂,其制造方法,使用该催化剂制造γ-丁内酯的方法,以利用废琥珀酸作为环境友好型产品。材料代替马来酸酐。组成:基于琥珀酸加氢制备γ-丁内酯的钯-氧化铝复合催化剂包括基于氧化铝和钯的化学键的Al-O-Pd结构。在复合催化剂中,钯的含量为氧化铝总重量的1至10重量%。络合催化剂的平均孔径在2nm至10nm之间。络合催化剂的表面积在10m 2 / g至400m 2 / g之间。复合催化剂的制造方法包括以下步骤:溶解铝前体,加入水和水合合成催化剂以形成氧化铝溶胶。将钯前体醇溶液加入氧化铝溶胶中,合成氧化铝-钯复合溶胶。冷却氧化铝-钯复合溶胶,并向冷却后的复合溶胶中加入水,得到钯-氧化铝复合凝胶。复合凝胶经过老化,干燥和增塑。

著录项

  • 公开/公告号KR101205789B1

    专利类型

  • 公开/公告日2012-11-28

    原文格式PDF

  • 申请/专利权人

    申请/专利号KR20100097476

  • 发明设计人 송인규;홍웅기;서정길;박선영;

    申请日2010-10-06

  • 分类号B01J23/44;B01J37/02;C07D307/33;

  • 国家 KR

  • 入库时间 2022-08-21 16:28:08

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号