PURPOSE: A polymer concrete composition and a manufacturing method thereof are provided to be environmentally friendly and economical. CONSTITUTION: A polymer concrete composition comprises 7-8.5 parts by weight of a polymer binder; 5-15 parts by weight of calcium carbonate; 6.63-19.89 parts by weight of quenching agent steel slag having a particle size of 0.1-0.5mm; 27.02 parts by weight of quenching agent steel slag having a particle size of 0.6-1.2mm; and 51.5-53 parts by weight of coarse aggregate having a particle size of 5-8mm. A manufacturing method of the polymer concrete composition comprises the following steps: mixing unsaturated polyester resin with polystyrene resin; mixing a catalyst, a cross-linking agent, and a promoter with the mixed resin; mixing calcium carbonate, coarse aggregate, and quenching agent steel slag; and adding the polymer binder to the powder mixture and stirring the same.
机译:目的:提供一种聚合物混凝土组合物及其制造方法,以环保和经济。组成:一种聚合物混凝土组合物包含7-8.5重量份的聚合物粘合剂。 5-15重量份的碳酸钙; 6.63-19.89重量份粒度为0.1-0.5mm的淬火剂钢渣; 27.02重量份的粒度为0.6-1.2mm的淬火剂钢渣; 51.5-53重量份的粒度为5-8mm的粗骨料。聚合物混凝土组合物的制造方法包括以下步骤:将不饱和聚酯树脂与聚苯乙烯树脂混合;和将不饱和聚酯树脂与聚苯乙烯树脂混合。将催化剂,交联剂和促进剂与混合树脂混合;混合碳酸钙,粗骨料和淬火剂钢渣;将聚合物粘合剂加入到粉末混合物中并搅拌。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号