PURPOSE: a kind of manufacture solid fuel using the purpose of paper mill sludge and house refuse be prevent from increasing by reducing waste water environmental pollution resource utilization efficiency it is waste and old by recycling, reduce production cost, use the raw material and low unit cost. ;CONSTITUTION: the manufacturing method of solid fuel comprises the steps of: filling dehydration paper sludge and wasting the anoxic incinerator of vacuum state and makes moisture content 80-90%; (S100) carbonization ash is formed by heating in 250-450& deg; C incinerates identical with vacuum from incinerator; (S200) charcoal ashing is crushed; (S300) one of production liquefaction coagulant is placed on carboxymethyl cellulose and kelp or natural plant gum is that water is identical with heating; (S400) 1-1. is mixedEvery 5kg carbonized dusts of 5L coagulant condense carbonized dust; (S500) being put into carbonized dust and having compressed with condensation briquetting pressure is 150-300 tons; (S600) it takes out the solid fuel of molding and completely removes moisture and pass through blowing 200-300& deg; The hot wind of C 15-30 minutes. ;The 2013 of copyright KIPO submissions;[Reference numerals] (S100) step forms carbonized dust; (S200) step crushes charcoal ashing; (S300) the manufacture coagulant of step; (S400) the coagulation charcoal ashing of step; (S500) time step compression forming; (S600) drying steps
机译:目的:通过减少废水,环境污染资源的利用效率来防止以造纸厂的污泥和房屋垃圾为目的生产固体燃料,通过回收利用来废旧,降低生产成本,使用原料,单位低等成本。组成:固体燃料的制造方法包括以下步骤:填充脱水纸污泥,浪费真空状态的缺氧焚化炉,使含水量达到80-90%。 (S100)通过在250-450℃下加热形成碳化灰。 C焚化炉中的真空度相同; (S200)木炭灰被粉碎; (S300)一种生产液化凝结剂置于羧甲基纤维素和海带或天然植物胶上,水与加热相同; (S400)1-1。每混合5L凝结剂的5kg碳化粉尘都会使碳化粉尘凝结; (S500)置于碳化粉尘中并经凝结压块压力压缩后为150-300吨; (S600)将成型的固体燃料取出,并完全除去水分,并通过200-300度吹气; C的热风15-30分钟。 ; 2013年版权KIPO提交文件; [参考数字](S100)步骤形成碳化粉尘; (S200)步骤粉碎木炭灰; (S300)步骤的制造凝结剂; (S400)混凝炭灰化步骤; (S500)时间步压缩成型; (S600)干燥步骤

著录项

  • 公开/公告号KR20130043810A

    专利类型

  • 公开/公告日2013-05-02

    原文格式PDF

  • 申请/专利权人 WI UN HYEOK;

    申请/专利号KR20110107929

  • 发明设计人 WI UN HYEOK;

    申请日2011-10-21

  • 分类号C10L5/40;B09B3/00;B30B11/00;C10B53/00;

  • 国家 KR

  • 入库时间 2022-08-21 16:27:16

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号