首页> 外国专利> WIRE FOR WIRE DRAWING WHICH HAS AN EXCELLENT WIRE DRAWING PROPERTY WITH HIGH SURFACE LUBRICATION, AND WIRE DRAWING METHOD THEREOF

WIRE FOR WIRE DRAWING WHICH HAS AN EXCELLENT WIRE DRAWING PROPERTY WITH HIGH SURFACE LUBRICATION, AND WIRE DRAWING METHOD THEREOF

机译:具有出色的高表面润滑性能的拉丝性能的拉丝方法及其拉丝方法

摘要

PURPOSE: A wire for wire drawing which has an excellent wire drawing property with high surface lubrication is provided to form a self-lubrication layer without any special coating on the surface of a steel material by including antimony.;CONSTITUTION: A wire for wire drawing which has an excellent wire drawing property is composed of, in wt%: C: 0.25-0.45; Si: 0.1-0.2; Mn: 0.1-0.7; Sb: 0.005-0.02; and the remainder Fe and inevitable impurities. The wire for wire drawing includes Sb oxide inside. The internal structure of the wire for wire drawing is composed of ferrite and pearlite, and the grain size of the ferrite is 20μm or less. A wire drawing method comprises the following steps of: preparing the wire for wire drawing; heating the wire at the temperature of 300-400°C; and drawing the wire.;COPYRIGHT KIPO 2013
机译:目的:提供一种具有优异的拉丝性能并具有高表面润滑性能的拉丝金属丝,以通过在其中包含锑而在钢材表面形成一层没有任何特殊涂层的自润滑层;组成:拉丝金属丝具有优良的拉丝性能的金属以重量%计由C:0.25-0.45组成。 Si:0.1-0.2; Si:0.1-0.2。锰:0.1-0.7;锑:0.005-0.02;其余的铁和不可避免的杂质。拉丝用线的内部含有Sb氧化物。拉丝用线的内部结构由铁素体和珠光体构成,铁素体的粒径为20μm以下。拉丝方法包括以下步骤:准备用于拉丝的线;在300-400℃的温度下加热电线;和画线。; COPYRIGHT KIPO 2013

著录项

  • 公开/公告号KR20130053084A

    专利类型

  • 公开/公告日2013-05-23

    原文格式PDF

  • 申请/专利权人 POSCO;

    申请/专利号KR20110118608

  • 发明设计人 LEE YOU HWAN;KIM DONG HYUN;

    申请日2011-11-15

  • 分类号C22C38/00;B21C1/00;

  • 国家 KR

  • 入库时间 2022-08-21 16:27:05