首页> 外国专利> METHOD FOR PRODUCTION OF GOLD NANOFLUIDS USING ULTRASONIC BATH

METHOD FOR PRODUCTION OF GOLD NANOFLUIDS USING ULTRASONIC BATH

机译:用超声波浴生产金纳米流体的方法

摘要

PURPOSE: A method of manufacturing a gold nano fluid using an ultrasonic generation water tank is provided to use a dispersion energy source which generates gold nano particles uniformly by preventing not only a chemical reaction but also thermal energy for activating a reduction reaction from being generated locally. CONSTITUTION: A method of manufacturing a gold nano fluid using an ultrasonic generation water tank comprises the following steps: a water temperature inside an ultrasonic water tank is maintained with 80 to 90°C; a chloroauric acid aqueous solution consisting of 0.25 mM of a molarity is put into a container; after the container is fixed inside the ultrasonic water tank, ultrasonic energy is given; a sodium citrate aqueous solution is injected within the container in order to make 1 : 3.5 of a molar fraction of a chloroauric acid and a sodium citrate in the chloroauric acid aqueous solution within the container; and the ultrasonic energy is given within the ultrasonic water tank again.
机译:目的:提供一种使用超声波发生水槽制造金纳米流体的方法,以使用分散能量源,该分散能量源通过不仅防止化学反应而且还防止局部产生用于激活还原反应的热能来均匀地产生金纳米颗粒。 。构成:一种使用超声波发生水箱制造金纳米流体的方法,包括以下步骤:将超声波水箱内的水温保持在80至90℃;将水温保持在80-90℃。将摩尔浓度为0.25mM的氯金酸水溶液放入容器中。将容器固定在超声波水箱内后,给予超声波能量。向容器内注入柠檬酸钠水溶液,以使容器内的氯金酸水溶液中的氯金酸和柠檬酸钠的摩尔分数为1:3.5。超声波能量再次在超声波水箱内提供。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号