首页> 外国专利> Reduction refining method of Phosphorus from MG-Si by strongly reducing slags

Reduction refining method of Phosphorus from MG-Si by strongly reducing slags

机译:通过强烈还原渣还原MG-Si中的磷的还原精制方法

摘要

A method for reducing and refining P in MG-Si using slag is provided. The present invention comprises the steps of adjusting the atmosphere of the refining crucible to a reducing gas atmosphere consisting of at least one inert gas selected from CCl 4 , CF 4 , Ar, He, N 2 and at least one reducing gas of H 2 and CO; An alkaline earth metal oxide composed of at least one of SiO 2 , CaO, MgO, and BaO such that the weight ratio of the MG-Si raw material, the MG-Si raw material, and the slag is 1: 1 to 3 in the crucible adjusted to the atmosphere; At least one alkali metal oxide of Na 2 O, K 2 O, Li 2 O; And charging the slag made of CaF 2 together; And heating the crucible to melt the charged MG-Si raw material and slag to remove P in the molten Si into slag in the form of Phosphide (P 3 ) ion through an interfacial reaction between molten Si and slag. .
机译:提供了一种使用炉渣还原和精制MG-Si中的P的方法。本发明包括以下步骤:将精炼坩埚的气氛调整为还原性气体气氛,所述还原性气体气氛由选自以下的至少一种惰性气体组成:CCl 4 ,CF 4 ,Ar, He,N 2 和至少一种H 2 和CO的还原气体;由SiO 2 ,CaO,MgO和BaO中的至少一种组成的碱土金属氧化物,使得MG-Si原料,MG-Si原料和炉渣的重量比在调整到大气的坩埚中为1:1到3; Na 2 O,K 2 O,Li 2 O中的至少一种碱金属氧化物;并将由CaF 2 制成的炉渣一起装填;然后加热坩埚以熔化带电的MG-Si原料和炉渣,以通过磷离子(P 3 -)的形式将熔融硅中的P去除为炉渣。熔融硅与炉渣之间的界面反应。 。

著录项

  • 公开/公告号KR101219759B1

    专利类型

  • 公开/公告日2013-01-08

    原文格式PDF

  • 申请/专利权人

    申请/专利号KR20100016459

  • 发明设计人 민동준;정은진;문병문;

    申请日2010-02-24

  • 分类号C30B25;C30B29/06;C01B33/037;C22B7/04;

  • 国家 KR

  • 入库时间 2022-08-21 16:25:56

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号