PURPOSE: A CuNi 90/10 flange and a method using free forging for manufacturing the same are provided to enable to form a regular alignment structure without heat-processing CuNi. CONSTITUTION: A method using free forging for manufacturing a CuNi 90/10 flange comprises; a step(S10) for preparing a continuous casting bar of a diameter of 6-10 inches; a step(S20) for cutting the continuous casting bar into 5-10 inches in a longitudinal direction; a step(S30) for heating the cut casting bar at a temperature of 900-950C for 150-300 minutes; a step(S40) for upsetting-forging the heated casting bar; a step(S50) for cogging the casting bar; a step(S60) for upsetting-forging the casting bar again after cogging; and a step(S70) for forming a flange shape by forging the casting rod. [Reference numerals] (S10) Preparing a casting bar material for 6-10 inches; (S20) Cutting a casting bar; (S30) Heating the casting bar(900-950C/30min); (S70) Generating a flange through die forging; (S80) Hole processing(Drilling or Punching)
机译:目的:提供一种CuNi 90/10法兰和一种使用自由锻造的方法来制造该法兰,以能够在不对CuNi进行热处理的情况下形成规则的对准结构。构成:一种使用自由锻造制造CuNi 90/10法兰的方法,包括:步骤(S10),用于制备直径为6-10英寸的连铸坯;步骤(S20),用于将连铸坯在纵向上切割成5-10英寸。步骤(S30),用于在900-950℃的温度下将切割的铸坯加热150-300分钟;步骤S40,用于up锻加热后的铸坯;步骤(S50),对铸棒进行齿槽加工;步骤(S60),在齿槽加工后再次up锻铸造棒;步骤(S70),其通过锻造铸造棒而形成凸缘形状。 [附图标记](S10)准备6-10英寸的铸条材料; (S20)切断铸坯; (S30)加热铸棒(900-950C / 30min); (S70)通过模锻产生凸缘; (S80)孔加工(钻孔或冲孔)

著录项

  • 公开/公告号KR101243436B1

    专利类型

  • 公开/公告日2013-03-13

    原文格式PDF

  • 申请/专利权人 SAMYANG METAL IND. CO. LTD.;

    申请/专利号KR20120130923

  • 发明设计人 SEO JIN MIN;

    申请日2012-11-19

  • 分类号B21J5/08;B21J5/12;B21K21;

  • 国家 KR

  • 入库时间 2022-08-21 16:25:34

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号