首页> 外国专利> HIGH VOLUME BLAST FURNACE SLAG CONCRETE COMPOSITION USING WASTE ASH AND RECYCLED AGGREGATE

HIGH VOLUME BLAST FURNACE SLAG CONCRETE COMPOSITION USING WASTE ASH AND RECYCLED AGGREGATE

机译:利用废灰和再生骨料的高容量高炉矿渣混凝土组合物

摘要

PURPOSE: High volume blast furnace slag concrete using incineration plant ash and recycled aggregate is provided to increase strength of concrete by accelerating a latent hydraulic activity of ground powder of blast furnace slag using the incineration plant ash and the recycled aggregate. CONSTITUTION: High volume blast furnace slag concrete comprises: a binding material; water; recycled small aggregate; and recycled big aggregate. The binding material comprises: 70-90wt% of ground powder of blast furnace slag; and 10-30wt% of normal Portland cement. The incineration plant ash substitutes for the cement, and is included in 0.5-2.0wt% to the binding material. A manufacturing method for the incineration plant ash comprises the following steps: Dust is collected by spraying milky lime to exhaust gas generated while incinerating city life garbage.; The milky lime is sprayed in a semi-dry alkali reaction tower in a form of lime slurry.; The high volume blast furnace slag concrete is mixed in a water binder ratio of 40-65wt% and a fine aggregate modulus of 35-50vol%. [Reference numerals] (AA) Compressive intensity(MPa); (BB) Material age(days)
机译:目的:使用焚化厂灰渣和再生骨料提供高容量的高炉矿渣混凝土,通过加速使用焚化厂灰烬和再生骨料的矿渣粉的潜在水硬性,从而提高混凝土强度。组成:高容量高炉矿渣混凝土包括:粘结材料;水;回收的小骨料;和回收的大骨料。粘结材料包括:70-90wt%的高炉渣磨粉;和和普通硅酸盐水泥的10-30wt%。焚烧厂的灰分代替水泥,占粘结材料的0.5-2.0wt%。焚烧植物灰的制造方法包括以下步骤:通过将乳白色石灰喷洒到焚化城市生活垃圾时产生的废气中来收集灰尘。乳状石灰以石灰浆的形式喷入半干碱反应塔中。将高容量高炉矿渣混凝土以40-65wt%的水粘合剂比率和35-50vol%的细骨料模量混合。 [参考数字](AA)抗压强度(MPa); (BB)物质年龄(天)

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号