PURPOSE: An iron-nickel/chrome-carbon nanotube metal separation plate is provided to have excellent intensity, hardness, durability, corrosion resistance and/or electric conductance. CONSTITUTION: An iron-nickel/chrome-carbon nanotube metal separation plate comprises an alloy of iron and nickel, and chrome and carbon nanotube-containing layers formed on both sides of an alloy thin-film of the iron and nickel. A flow path shape of the separation plate for a fuel cell is formed in the iron-nickel/chrome-carbon nanotube metal separation plate. The alloy thin-film of the iron and nickel has a thickness of 30-70 um and comprises 5-30 wt% of nickel and a remaining content of iron and other unavoidable impurities. The chrome and carbon nanotube-containing layer has a thickness of 0.1-20 um and comprises 10-50 wt% of carbon nanotubes and a remaining content of chrome and other unavoidable impurities.
机译:目的:提供一种铁镍/铬碳纳米管金属隔板,具有出色的强度,硬度,耐用性,耐腐蚀性和/或电导率。组成:铁-镍/铬-碳纳米管金属隔板包括铁和镍的合金,以及在铁和镍的合金薄膜的两侧形成的含铬和碳纳米管的层。在铁-镍/铬-碳纳米管金属隔板中形成用于燃料电池的隔板的流路形状。铁和镍的合金薄膜具有30-70 um的厚度,并且包含5-30 wt%的镍以及剩余的铁和其他不可避免的杂质。含铬和碳纳米管的层的厚度为0.1-20μm,并包含10-50wt%的碳纳米管和剩余含量的铬和其他不可避免的杂质。

著录项

  • 公开/公告号KR101262600B1

    专利类型

  • 公开/公告日2013-05-08

    原文格式PDF

  • 申请/专利权人 POSCO;

    申请/专利号KR20110142318

  • 申请日2011-12-26

  • 分类号H01M8/02;C23C28;C25D1;H01M8/10;

  • 国家 KR

  • 入库时间 2022-08-21 16:25:14

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号