PURPOSE: An eco-friendly flame-resistant foaming deck material and a manufacturing method for the same are provided to improve high intensity and eco-friendly properties by adding eco-friendly filler to high density polyethylene and to obtain the flexibility a porous structure using a foaming agent. CONSTITUTION: A manufacturing method of an eco-friendly flame-resistant foaming deck material comprises the following steps: putting high density polyethylene in an eco-friendly flame-resistant foaming composition into a mixture machine for melting; injecting a foaming agent in the composition into the melted high density polyethylene and injecting a foaming accelerant in the composition; adding a filler, a cross-linking agent, an antioxidant, an UV stabilizer, a flame retardant, an inorganic pigment, a lubricant, and a dispersing agent in the composition and mixing for 20 minutes; molding the mixed composition in an extruder for forming a deck material and brushing the deck material; and cutting the deck material into desired sizes and shapes. [Reference numerals] (AA) Step of preparing a composition on the table 1 according to a weight ratio; (BB) Step of melting the high density polyethylene of the composition; (CC) Step of injecting a foaming agent; (DD) Step of injecting a foaming accelerant; (EE) Step of adding a filler, a cross-linking agent, an antioxidant, an UV stabilizer, a flame retardant, an inorganic pigment, a lubricant, and a dispersing agent in the composition to mix; (FF) Step of forming a deck material by molding the mixed composition in an extruder; (GG) Step of brushing the deck material; (HH) Step of cutting the deck material
机译:用途:提供一种环保型阻燃发泡甲板材料及其制造方法,以通过向高密度聚乙烯中添加环保填料来提高高强度和环保性能,并通过使用发泡剂。组成:一种环保阻燃发泡甲板材料的制造方法包括以下步骤:将高密度聚乙烯在环保阻燃发泡组合物中放入混合机中进行熔融;将组合物中的发泡剂注入熔融的高密度聚乙烯中,并向组合物中注入发泡促进剂;在组合物中加入填料,交联剂,抗氧化剂,紫外线稳定剂,阻燃剂,无机颜料,润滑剂和分散剂并混合20分钟;在挤出机中模制混合的组合物以形成甲板材料并刷涂甲板材料;并将甲板材料切成所需的尺寸和形状。 [附图标记](AA)根据重量比在桌子1上制备组合物的步骤; (BB)熔融组合物的高密度聚乙烯的步骤; (CC)注入发泡剂的步骤; (DD)注入发泡促进剂的步骤; (EE)在组合物中添加填料,交联剂,抗氧化剂,紫外线稳定剂,阻燃剂,无机颜料,润滑剂和分散剂的步骤。 (FF)通过在挤出机中模制混合的组合物形成甲板材料的步骤; (GG)刷甲板材料的步骤; (HH)切割甲板材料的步骤

著录项

  • 公开/公告号KR101285869B1

    专利类型

  • 公开/公告日2013-07-12

    原文格式PDF

  • 申请/专利权人 MK WOOD;

    申请/专利号KR20120061160

  • 发明设计人 BAEK HYEON SU;

    申请日2012-06-07

  • 分类号E04F15/02;E01C5;E04B1;

  • 国家 KR

  • 入库时间 2022-08-21 16:24:49

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号