Heterostructure nanowires with intermetallic or alloy core and carbon nanotube shell, and manufacturing method thereof

机译:具有金属间或合金核和碳纳米管壳的异质结构纳米线及其制造方法

摘要

PURPOSE: A hetero-nanowire consisting of intermetallic compound or alloy core and carbon nanotube shell and a synthesizing method are provided to include inter metallic compound or alloy inside the wire by uniformly mixing metal oxides and controlling compound condition. CONSTITUTION: A synthesizing method of a hetero-nanowire consisting of intermetallic compound or alloy core comprises the following steps: putting metal oxide compound into a reactor; eliminating remnant oxygen within the reactor by lowering degree of vacuum; injecting carrier gas under a vacuum atmosphere; increasing internal temperature of the reactor to a reaction temperature; injecting hydrocarbon gas into the reactor; and reacting the hydrocarbon gas with the metal oxide compound. The metal oxide compound is a mixture of tin oxide and indium oxide. A mixing ratio of the tin oxide to the indium oxide is 6:1-1:6 in weight ratio. The reaction with the metal oxide compound with the hydrocarbon gas is processed at 550-850 deg Celsius and lasts within 2 hours.
机译:目的:提供一种由金属间化合物或合金核和碳纳米管壳组成的杂纳米线及其合成方法,通过均匀混合金属氧化物并控制化合物条件,在金属丝内部包括金属间化合物或合金。组成:一种由金属间化合物或合金核组成的杂纳米线的合成方法,包括以下步骤:将金属氧化物化合物放入反应器中;通过降低真空度消除反应器内的残留氧气;在真空气氛下注入载气;将反应器的内部温度提高到反应温度;向反应器中注入烃气;使烃类气体与金属氧化物化合物反应。金属氧化物化合物是氧化锡和氧化铟的混合物。氧化锡与氧化铟的混合比以重量比计为6:1-1:6。与金属氧化物化合物与烃类气体的反应在550-850摄氏度下进行并持续2小时。

著录项

  • 公开/公告号KR101308420B1

    专利类型

  • 公开/公告日2013-09-16

    原文格式PDF

  • 申请/专利权人

    申请/专利号KR20100110445

  • 发明设计人 정남조;여정구;

    申请日2010-11-08

  • 分类号B82B3;B82B1;

  • 国家 KR

  • 入库时间 2022-08-21 16:24:28

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号