首页> 外国专利> METHOD OF PRODUCING COMPOSITE BINDER, COMPOSITE BINDER FOR PRODUCING MOULDED AUTOCLAVE HARDENING ARTICLES, MOULDED ARTICLE

METHOD OF PRODUCING COMPOSITE BINDER, COMPOSITE BINDER FOR PRODUCING MOULDED AUTOCLAVE HARDENING ARTICLES, MOULDED ARTICLE

机译:复合粘合剂的制造方法,用于制造高压灭菌硬模制品的复合粘合剂,模制品

摘要

FIELD: chemistry.;SUBSTANCE: invention relates to the building industry and can be used to produce silica brick and moulded autoclave hardened wall materials. The method of producing composite binder for producing moulded articles involves pre-slaking highly active lime with water to lime ratio equal to 0.48, in the presence of a gypsum dihydrate additive in amount of 0.05-0.25% of the mass of lime, followed by mixing the obtained lime binder with ground quartz sand in the following ratio, wt %: lime binder 33.3-50, ground quartz sand - the balance. The composite binder is characterised by that it is obtained using the method described above. The moulded article in form of silica brick is characterised by that when using the binder described above, said brick is obtained from a mixture containing the following, wt %: said binder 10-30, non-ground quartz sand 70-90.;EFFECT: wider range of means of producing moulded autoclave hardened articles, having high strength, low cost of production by cutting power consumption when producing the binder and articles based thereon, and controlling lime slaking, dispersity of the binder.;3 cl, 2 tbl, 1 ex, 1 dwg
机译:发明领域本发明涉及建筑工业,可用于生产硅砖和模压高压釜硬化的墙体材料。生产用于生产模制品的复合粘合剂的方法包括在水合石膏质量为石灰质量的0.05-0.25%的情况下,以水与石灰之比等于0.48的方式预研磨高活性石灰。所得到的石灰粘合剂与石英砂的重量比如下:wt%:石灰粘合剂33.3-50,石英砂-余量。复合粘合剂的特征在于它是使用上述方法获得的。二氧化硅砖形式的模制品的特征在于,当使用上述粘合剂时,所述砖由包含以下重量%的混合物获得:所述粘合剂10-30,非研磨石英砂70-90。 :生产模压高压灭菌硬化制品的方法范围更广,具有高强度,通过降低生产粘结剂和基于粘结剂的制品时的功耗并控制石灰剥落,粘结剂的分散性而降低了生产成本; 3 cl,2 tbl, 1 ex,1 dwg

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号