FIELD: chemistry.;SUBSTANCE: method involves defatting, washing in hot flowing water, washing in cold flowing water, activating, washing in cold flowing water, washing in two collectors, washing in cold flowing water and drying. Activation is carried out in a solution of the following composition, g/l: sodium hypophosphite 8-12, hydrofluoric acid 2-6, distilled water - up to 1 l, pH 2.7, at temperature of +10 - +20°C for 10 minutes, and after activating and washing in cold flowing water, the silver precoating and basic coating are applied in a solution of the following composition, g/l: silver nitrate 15-25, potassium ferrocyanide 25-30, anhydrous sodium carbonate 10-15, water - up to 1 l. The silver precoating is applied at temperature of +18 - +25°C for 10 minutes with current density of 0.025 A/dm2, and the basic silver coating is applied at temperature of +18 - +25°C with current density of 0.1 A/dm2.;EFFECT: shorter process cycle.;3 ex
机译:领域:化学;物质:该方法涉及脱脂,在热流动水中洗涤,在冷流动水中洗涤,活化,在冷流动水中洗涤,在两个收集器中洗涤,在冷流动水中洗涤并干燥。在以下组成的溶液中进行活化:g / l:次磷酸钠8-12,氢氟酸2-6,蒸馏水-最高1 l,pH 2.7,温度+10-+ 20°C 10分钟后,在冷水中活化和洗涤后,将银预涂层和碱性涂层以以下组成的溶液g / l涂覆:硝酸银15-25,亚铁氰化钾25-30,无水碳酸钠10- 15,水-最多1升。在+18-+ 25°C的温度下以10分钟的电流密度0.025 A / dm 2 施加银预涂层,在+18-+25的温度下施加基础银涂层°C,电流密度为0.1 A / dm 2 。;效果:工艺周期更短; 3 ex

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号