A method for rolling thin and / or thick slabs (2, 3) made of steel materials to form hot strip (4a), the previously as a thin or thickness of slabs (2, 3) in a continuous casting machine (1) have been cast, in a tunnel furnace (5) or a lifting beam furnace (6) and heated to rolling temperature in a rolling mill train (4) are rolled, then cooled and connected to coil (18) are wound,in the:(A) is made of an individual thin slabs - continuous casting machine (1), the an existing rolling mill train (4) is arranged in front of or is arranged, continuously coming one behind the thin slabs - sections (2b), which consists of the tunnel kiln (5), or(B) transversely into the rolling mill train is introduced (4) thick or thin slabs - portions (3b, 2b), which consist of the strike beam furnace (6) escape,(C) directly in the thickness (9) reducing roughing stands (4c) or(D) not be rolled by roughing stands (4c) or directly, before the first roll stand of the finishing train (12) and guided(E) in the with the roughing stands (4c) in a rolling line (4) lying..