PROBLEM TO BE SOLVED: To provide a negative electrode active material of high crystallinity, high uniformity and high purity self-supporting metal sulfide-based two-dimensional nanostructure applicable to a secondary battery, and to provide a production method therefor.SOLUTION: The negative electrode active material grows directly, as a metal sulfide-based two-dimensional nanostructure, on a metal substrate by peeling an aggregate composed of a metal sulfide-based material. The production method thereof includes a step for producing an aggregate composed of a metal sulfide-based material, a step for inserting the aggregate into a tube in an electric furnace for pulse laser vapor deposition, a step for inserting a metal substrate into a tube and locating the metal substrate separately from the aggregate, a step for lowering the pressure in the tube to vacuum state and raising the temperature of the electric furnace to 590-610°C, and a step for peeling the aggregate by injecting pulse laser into the tube. The metal sulfide-based material is grown, as a two-dimensional nanostructure, directly on the metal substrate.
机译:解决的问题:提供适用于二次电池的,具有高结晶度,高均匀性和高纯度的自支撑金属硫化物基二维纳米结构的负极活性材料,并提供其制备方法。通过剥离由金属硫化物基材料构成的聚集体,电极活性材料作为金属硫化物基二维纳米结构直接在金属基板上生长。其生产方法包括以下步骤:生产由金属硫化物基材料组成的聚集体;将聚集体插入电炉中用于脉冲激光气相沉积的管中的步骤;将金属基板插入管中的步骤;和将金属基板与骨料分开放置,将管中的压力降低至真空状态并将电炉的温度升高至590-610°C的步骤,以及通过将脉冲激光注入管中来剥离骨料的步骤。基于金属硫化物的材料作为二维纳米结构直接在金属基板上生长。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号