首页> 外国专利> Wall measuring method of the carbonization chamber of coke oven , wall measuring device of the carbonization chamber of coke oven , and a computer program

Wall measuring method of the carbonization chamber of coke oven , wall measuring device of the carbonization chamber of coke oven , and a computer program

机译:焦炉碳化室壁测量方法,焦炉碳化室壁测量装置和计算机程序

摘要

PROBLEM TO BE SOLVED: To accurately extract the image of laser spots in measuring the unevenness levels of the wall surface of the carbonizing chamber of a coke oven, based on such an image in which the images of the laser spots and that of the oven wall are superimposed on each other through irradiating the wall of the carbonizing chamber of the coke oven with laser beams while moving the laser beams in the direction of oven length relative to the wall of the carbonizing chamber of the coke oven.;SOLUTION: Using a wall surface-observing apparatus 100, the oven wall 14 of a carbonizing chamber 11 is irradiated with laser beams while moving the laser beams toward the depth direction to acquire such "an image of the oven wall 14" that images of the laser spots 42 are superimposed on each other; wherein, the laser beams irradiation is made in such a way that the width (the length of the carbonizing chamber 11 in its height direction) of a line segment (laser line segment 601) extended toward the depth direction of the laser spots 42 is shorter than the width of each of the joints 602 of the refractory bricks. Subsequently, a laser line segment-intensifying treatment is performed so that only the luminance in a high-luminance region with a width same as that supposed as the line segment (laser line segment 601) extended toward the depth direction of the laser spots 42 is made higher than the original luminance, followed by performing a laser line segment 601 follow-up treatment.;COPYRIGHT: (C)2012,JPO&INPIT
机译:解决的问题:基于这样的图像,在测量焦炉碳化室壁表面的不平整度时,要准确地提取激光斑点的图像,其中激光斑点和烤箱壁的图像通过用激光束照射焦炉的碳化室壁而使它们彼此重叠,同时沿相对于焦炉的碳化室壁的炉子长度方向移动激光束。在表面观察装置100中,一边使激光束向深度方向移动,一边向碳化室11的炉壁14照射激光,从而获得激光斑点42的图像重叠的“炉壁14的图像”。彼此其中,以使沿激光点42的深度方向延伸的线段(激光线段601)的宽度(碳化室11的高度方向上的长度)短的方式进行激光照射。宽度大于耐火砖的每个接缝602的宽度。随后,执行激光线段增强处理,使得仅具有与假定为朝着激光点42的深度方向延伸的线段(激光线段601)相同的宽度的高亮度区域中的亮度。使其高于原始亮度,然后执行激光线段601的后续处理。;版权所有:(C)2012,JPO&INPIT

著录项

  • 公开/公告号JP5569318B2

    专利类型

  • 公开/公告日2014-08-13

    原文格式PDF

  • 申请/专利权人 新日鐵住金株式会社;

    申请/专利号JP20100226851

  • 发明设计人 杉浦 雅人;藤懸 洋一;

    申请日2010-10-06

  • 分类号C10B29/06;C10B29/02;F27D1/00;F27D21/00;F27D21/02;G01B11/24;G01N21/954;

  • 国家 JP

  • 入库时间 2022-08-21 16:15:53