摘要

PROBLEM TO BE SOLVED: To suppress a Pb elution amount within an environmental standard without elevating manufacturing costs in a slag for a roadbed material.;SOLUTION: The slag for a roadbed material is obtained by pulverizing a steel slag containing Pb of 0.1 ppm or more and a basicity of the steel slag (CaO/SiO2) is 1.5 or more. The slag for the roadbed material has a particle size distribution which a mass ratio occupied by the slag particle having a particle size of 100 μm or less to all slag particles after pulverization is 0.5 wt.% to 3.5 wt.% and satisfies the relations that the product of the mass ratio occupied by the slag particle having 100 μm or less and the Pb concentration of the slag particle after pulverization (ppm) is 15 or less.;COPYRIGHT: (C)2014,JPO&INPIT
机译:解决的问题:在不增加路基材料炉渣制造成本的情况下,在环境标准范围内抑制Pb的溶出量;解决方案:路基材料炉渣是通过将0.1 Pb或更高的Pb钢渣粉碎而获得的钢渣(CaO / SiO 2 )的碱度为1.5以上。用于路基材料的炉渣具有粒径分布,其中粒径为100μm或更小的炉渣颗粒在粉碎后相对于所有炉渣颗粒的质量比为0.5重量%至3.5重量%,并且满足以下关系:小于100μm的炉渣颗粒所占的质量比与粉化后的炉渣颗粒的Pb浓度(ppm)的乘积为15以下。版权所有:(C)2014,JPO&INPIT

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号