首页> 外国专利> As at least 1 kinds of production methodological null all the ratio solid solution type stabilization elements of high intensity + type titanium

As at least 1 kinds of production methodological null all the ratio solid solution type stabilization elements of high intensity + type titanium

机译:作为至少一种生产方法无效的高强度+型钛全比例固溶型稳定元素

摘要

PROBLEM TO BE SOLVED: To provide an α+β type titanium alloy plate which is highly strong and is also excellent in strength anisotropy.;SOLUTION: The high strength α+β type titanium alloy plate contains 2.0-4.5 mass% of at least one of all proportional solid solution type β stabilizing elements by Mo equivalent, 0.3-2.0 mass% of at least one of eutectoid type β stabilizing elements by Fe equivalent, and over 3 mass% and not more than 5.5 mass% of at least one of α stabilizing elements by Al equivalent, and further contains 0.1-1.5 mass% of Si, 0.01-0.15 mass% of C, and the balance being Ti and inevitable impurities. The average value of an inclination angle formed by a normal of (0001) surface of an α phase and a normal of a rolling surface is equal to or smaller than 60°, and the area ratio of the α phase for which the inclination angle is equal to or larger than 70° to the entire α phase is equal to or lower than 40%.;COPYRIGHT: (C)2012,JPO&INPIT
机译:要解决的问题:提供α +β高强度且强度各向异性也优异的钛型钛合金板。型钛合金板包含2.0-4.5质量%的所有比例固溶体类型β中的至少一种。稳定元素按Mo当量计,共析型β的至少一种为0.3〜2.0质量%。稳定元素按Fe当量计,且大于或等于3质量%且不大于5.5质量%的α中的至少一种。稳定元素按Al当量计,还含有0.1〜1.5质量%的Si,0.01〜0.15质量%的C,其余为Ti和不可避免的杂质。由α的(0001)面的法线形成的倾斜角的平均值。相和滚动表面的法线等于或小于60°,并且α的面积比等于或小于60°。倾斜角等于或大于70°的相位;整个α相位等于或小于40%。;版权:(C)2012,日本特许厅&INPIT

著录项

  • 公开/公告号JP5421873B2

    专利类型

  • 公开/公告日2014-02-19

    原文格式PDF

  • 申请/专利权人 株式会社神戸製鋼所;

    申请/专利号JP20100172463

  • 发明设计人 逸見 義男;工藤 健;

    申请日2010-07-30

  • 分类号C22C14/00;C22F1/18;C22F1/00;

  • 国家 JP

  • 入库时间 2022-08-21 16:12:42

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号