PROBLEM TO BE SOLVED: To provide a polymerization method for an acrylic latex without emulsifier, having uniformly distributed particle diameters and excellent outward appearance of coating, and excellent in storage stability, permeability, a coating property, water resistance, tensile strength, and abrasion resistance.;SOLUTION: A reaction system is formed from 40-60 wt.% of pure water and 2-9 wt.% of a carboxylic acid monomer with a carbon-carbon double bond polymerizable functional group (A), and 40-50 wt.% of an alkyl methacrylate or an alkyl acrylate monomer (B), and 0.2-2.0 wt.% of an inorganic alkaline solution is first used to adjust the pH value of the reaction system to within a pH range of 9.0-13.0, then 0.2-1.0 wt.% of peroxide sulfate is used as initiators, and emulsification polymerization is carried out. At the end of the reaction, an organic amine compound is used to adjust the pH value of the obtained aqueous resin latex to within the pH range 7.0-9.5.;COPYRIGHT: (C)2012,JPO&INPIT
机译:解决的问题:提供不具有乳化剂的丙烯酸胶乳的聚合方法,该方法具有均匀分布的粒径和优异的涂层外观,并且具有优异的储存稳定性,渗透性,涂层性能,耐水性,拉伸强度和耐磨性解决方案:反应系统由40-60 wt。%的纯水和2-9 wt。%的具有碳-碳双键可聚合官能团(A)的羧酸单体和40-50 wt%的羧酸形成首先使用0.5%的甲基丙烯酸烷基酯或丙烯酸烷基酯单体(B)和0.2-2.0wt。%的无机碱性溶液将反应体系的pH值调节至9.0-13.0的pH范围内,然后使用0.2-1.0重量%的过氧化物硫酸盐作为引发剂,并进行乳化聚合。反应结束时,使用有机胺化合物将所得水性树脂胶乳的pH值调节至7.0-9.5范围内。版权所有:(C)2012,JPO&INPIT

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号