Method of making copper wire rod with low semi-softening temperature, method of making copper wire and copper wire

机译:半软化温度低的铜线材的制造方法,铜线及铜线的制造方法

摘要

A method of making a copper wire rod with low semi-softening temperature includes melting a raw material copper to have a copper melt, adjusting concentrations of oxygen and sulfur included in the copper melt to be not more than 20 ppm and not more than 6 ppm, respectively, continuously casting the adjusted copper melt at temperature not higher than 1120° C. to have a cast bar, and hot-rolling the cast bar in a temperature range of 850° C. to 550° C.
机译:一种半软化温度低的铜线材的制造方法,其特征在于,使原料铜熔融而形成铜熔液,将铜熔液中所含的氧和硫的浓度调整为20ppm以下且6ppm以下。分别在不高于1120℃的温度下连续铸造调整后的铜熔体以具有铸锭,并且在850℃至550℃的温度范围内对铸锭进行热轧。

著录项

  • 公开/公告号US8596333B2

    专利类型

  • 公开/公告日2013-12-03

    原文格式PDF

  • 申请/专利权人 SEIGI AOYAMA;TORU SUMI;

    申请/专利号US20100659453

  • 发明设计人 SEIGI AOYAMA;TORU SUMI;

    申请日2010-03-09

  • 分类号B22D11/00;C22B15/00;

  • 国家 US

  • 入库时间 2022-08-21 15:59:31