首页> 外国专利> A method for producing precursor fibers containing chlor-alkali for the production of carbon fibers, including a solution of at least one enzyme and a fibre polymer in at least one solvent, which is then insulated and transferred to a solidification tank. Solving problems with yarn nozzles, precursor fibers and carbon fibers

A method for producing precursor fibers containing chlor-alkali for the production of carbon fibers, including a solution of at least one enzyme and a fibre polymer in at least one solvent, which is then insulated and transferred to a solidification tank. Solving problems with yarn nozzles, precursor fibers and carbon fibers

机译:一种用于生产用于生产碳纤维的包含氯碱的前体纤维的方法,该方法包括将至少一种酶和纤维聚合物在至少一种溶剂中的溶液,然后将其绝缘并转移至固化槽。解决纱线喷嘴,前体纤维和碳纤维的问题

摘要

Producing a lignin-containing precursor fiber for producing carbon fibers and/or activated carbon fibers, comprises (a) providing a solution comprising at least one kind of lignin and at least one fiber-forming polymer in at least one solvent, and (b) introducing the solution into a coagulation bath by extruding through a spinneret, where the lignin precursor fiber precipitates. Independent claims are also included for: (1) the precursor fiber for producing carbon fibers comprising (in wt.%) at least one kind of lignin (10, 20-60), at least one kind of fiber-forming polymer (90, preferably 40-80), optionally a strength of at least 10 cN/tex, preferably at least 20 cN/tex, and/or optionally an modulus of elasticity of at least 1000 cN/tex, preferably at least 1300 cN/tex; (2) producing the carbon fiber, comprising stabilizing the precursor fiber at 100-400[deg] C, and carbonizing at greater than 800[deg] C under inert conditions; and (3) the carbon fiber produced by the above method.
机译:制备用于生产碳纤维和/或活性碳纤维的含木质素的前体纤维包括:(a)提供在至少一种溶剂中包含至少一种木质素和至少一种成纤聚合物的溶液,和(b)通过挤出通过喷丝板将溶液引入混凝浴,木质素前体纤维在此处沉淀。还包括以下独立权利要求:(1)用于生产碳纤维的前体纤维,其包含(以重量%计)至少一种木质素(10、20-60),至少一种成纤聚合物(90,优选40-80),任选地强度为至少10cN / tex,优选地至少20cN / tex,和/或任选地弹性模量为至少1000cN / tex,优选地至少1300cN / tex; (2)生产碳纤维,包括将前体纤维稳定在100-400℃,并在惰性条件下在大于800℃碳化。 (3)通过上述方法制造的碳纤维。

著录项

  • 公开/公告号CL2013003236A1

    专利类型

  • 公开/公告日2014-05-23

    原文格式PDF

  • 申请/专利权人 STORA ENSO OYJ;

    申请/专利号CL20130003236

  • 申请日2013-11-12

  • 分类号D01D5/06;D01F2/00;D01F9/17;

  • 国家 CL

  • 入库时间 2022-08-21 15:58:28