首页> 外国专利> Hydrometallurgical method for the Recovery of zinc in Sulphuric Acid from zinc sulfide concentrates with high iron content

Hydrometallurgical method for the Recovery of zinc in Sulphuric Acid from zinc sulfide concentrates with high iron content

机译:从高铁含量的硫化锌精矿中回收硫酸中锌的湿法冶金方法

摘要

Refers to a hydrometallurgical method for the Recovery of zinc in Sulphuric Acid from zinc sulfide concentrates with High Content of IronWhich includes: (a) a part of the Roasting of zinc Concentrate; (b) where the neutral leaching dissolves zinc oxide; c) acid leaching of zinc ferrites by using Concentrated sulfuric acid as electrolyte and exhausted, generating a solution that contains (i) between 10 and 35 g / l Fe + + +, (ii) between 10 and 70 g / l Sulphuric Acid,(iii) a residue where the lead, Silver and Gold, and (iv) a solution of zinc and iron; (d) Reducing the Fe + + + contained in the previous Stage Fe + + by adding zinc Concentrate; e) neutralizing the acidity in the resulting solution with calcine, generating a final solution With a pH from 3.8 to 5.2; (f) Iron oxidation and precipitation of jarosite in the resulting Solution free of Solid Pollutants, through the Injection of oxygen and the addition of an Alkali or Salt of Na +, NH4 +, resulting in a solution with a pH of 1.5 and 10 g / l acidity
机译:指从铁含量高的硫化锌精矿中回收硫酸中锌的湿法冶金方法,其中包括:(a)焙烧锌精矿的一部分; (b)中性浸出溶解氧化锌的地方; c)通过使用浓硫酸作为电解质并抽空铁酸锌,进行酸浸处理,生成一种溶液,其中含有(i)10至35 g / l Fe + +,(ii)10至70 g / l硫酸,(iii)铅,银和金的残留物,以及(iv)锌和铁的溶液; (d)通过添加精矿锌减少前一阶段中的Fe + +; e)用煅烧中和所得溶液的酸度,产生pH为3.8-5.2的最终溶液; (f)通过注入氧气并添加碱或Na +,NH 4 +的碱或盐,在所得的不含固体污染物的溶液中进行铁的氧化和黄铁矿的沉淀,得到的溶液的pH值为1.5和10 g酸度

著录项

  • 公开/公告号PE04272014A1

    专利类型

  • 公开/公告日2014-04-10

    原文格式PDF

  • 申请/专利权人 TAM 5 S.L.;

    申请/专利号PE20130002082

  • 发明设计人 TAMARGO GARCIA FRANCISCO JOSE;

    申请日2012-07-16

  • 分类号C22B1/02;C22B3/00;C22B19/20;

  • 国家 PE

  • 入库时间 2022-08-21 15:56:45