Styrene resin composition low surface gloss comprising: (A) 80 to 99.9% by weight of a basic resin comprising (a) polymer-modified styrene rubber and (b) a styrene unmodified gum ; (B) 0.1-20% by weight of a syndiotactic polystyrene having a melting point range 260 to 280 ° C as matting agent; and (C) a hydrogenated styrene block copolymer comprising styrene and butadiene rubber block block as a compatibilizer in an amount of 0.1-20% by weight to the total weight of the styrene resin low surface gloss comprising (A ) the base resin and (B) the matting agent; wherein the modified styrene polymer rubber (a) contains 5 to 30% by weight of a gum, 40-90% by weight of a styrene monomer and 5-30% by weight of an ethylenically unsaturated compound and styrene unmodified rubber (b) is prepared by copolymerizing a styrene monomer and an ethylenically unsaturated compound.
机译:苯乙烯树脂组合物的低表面光泽度,其包含:(A)80至99.9重量%的碱性树脂,包括(a)聚合物改性的苯乙烯橡胶和(b)苯乙烯未改性的胶; (B)0.1-20重量%的间规聚苯乙烯作为消光剂,其熔点在260至280℃之间; (C)氢化苯乙烯嵌段共聚物,其包含苯乙烯和丁二烯橡胶嵌段嵌段作为增容剂,其含量为苯乙烯树脂低表面光泽剂总重量的0.1-20重量%,其包含(A)基础树脂和(B) )消光剂;其中改性苯乙烯聚合物橡胶(a)包含5至30重量%的树胶,40至90重量%的苯乙烯单体和5至30重量%的烯键式不饱和化合物,并且苯乙烯未改性的橡胶(b)为通过使苯乙烯单体和烯键式不饱和化合物共聚制备。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号