摘要

Provided is a method for preparing quantum dots of lead selenide, comprising the following steps: 1) mixing selenium powder with octadecene, heating with stirring to dissolve the selenium powder fully, maintaining the temperature, then cooling to room temperature to obtain a stock solution of selenium; 2) mixing lead compound, oleic acid, octadecene and benzophenone together, and dissolving to obtain a stock solution of lead, then maintaining the temperature at 130-190°C; 3) adding the stock solution of selenium into the stock solution of lead rapidly, and maintaining the temperature at 100-160°C, after cooling, quantum dots of lead selenide are initially prepared; 4) adding the initially prepared quantum dots of lead selenide into a mixture of toluene and methanol, centrifugating and the supernatant to obtain a precipitate, then redissolving the precipitate with toluene to obtain a transparent solution of quantum dots of pure lead selenide. The method is safe in operation, simple, good in reproducibility and low in cost.
机译:提供一种制备硒化铅量子点的方法,包括以下步骤:1)将硒粉与十八碳烯混合,搅拌加热,使硒粉充分溶解,保持温度,然后冷却至室温,得到硒化铅的原液。硒; 2)将铅化合物,油酸,十八烯和二苯甲酮混合在一起,溶解得到铅储备液,然后保持温度在130-190℃; 3)将硒的母液迅速加入铅的母液中,并保持温度在100-160℃,冷却后,首先制备硒化铅的量子点; 4)将最初制备的硒化铅量子点添加到甲苯和甲醇的混合物中,离心分离并上清液以获得沉淀,然后用甲苯将沉淀再溶解以获得纯硒化铅量子点的透明溶液。该方法操作安全,简单,重复性好,成本低。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号