The present invention relates to a method for manufacturing a coated fabric for sailcloth. The coated fabric for sailcloth is manufactured by subjecting a fabric for sailcloth consisting of an ultra high-molecular polyethylene fiber and a high-strength polyester fiber to pretreatment, curing, tentering, resin coating, and thermosetting. In order to prevent the deterioration in physical properties of the ultra high-molecular weight polyethylene fiber, the curing treatment is performed at a temperature of 130-140, which is relatively lower than the curing temperature of the general high-strength polyester textile. Considering the deterioration in setting characteristics of the high-strength polyester due to the curing treatment, the width widening is minimized at the time of tentering and the thermosetting is conducted at a temperature of 100 or lower. The process for manufacturing a coated fabric for sailcloth of the present invention can effectively prevent the deterioration in physical properties of the ultra high-molecular weight polyethylene fiber contained in the coated fabric for sailcloth and effectively prevent the slow reduction in the width of the coated fabric for sailcloth during storage.
机译:本发明涉及一种用于帆布的涂层织物的制造方法。通过对由超高分子聚乙烯纤维和高强度聚酯纤维组成的船用织物进行预处理,固化,拉幅,树脂涂覆和热固性,来制造船用涂层织物。为了防止超高分子量聚乙烯纤维的物理性能变差,在130-140℃的温度下进行固化处理,该温度相对于一般的高强度聚酯纺织品的固化温度而言相对较低。考虑到由于固化处理引起的高强度聚酯的固化特性的劣化,在拉幅时宽度的宽度最小化,并且在100℃或更低的温度下进行热固性。本发明的帆艇用涂层布的制造方法可以有效地防止帆布用涂层布所含的超高分子量聚乙烯纤维的物性降低,并且可以有效地防止涂层布的宽度缓慢减小。存放期间用于帆布。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号