The present invention relates to a method for preparing bay salt capable of removing harmful materials and increasing healthful ingredients, by burning the bay salt. The preparation method according to the present invention comprises the following steps: (a) filling a red clay pottery with bay sa (b) heating a red clay kiln to a temperature of 1000-1400C by using hardwood charcoal; (c) placing the red clay pottery containing the bay salt on the heated red clay kiln; (d) after placing the red clay pottery on the kiln, oxidizing Na and Cl ingredients contained in the bay salt and then heating the red clay pottery for 7-10 minutes at the same temperature to thereby burn the bay salt to supplement with salt of inorganic components; and (e) after step (d), taking out the red clay pottery containing the burned bay salt from the red clay kiln. Accordingly, the bay salt prepared through heating at 1000-1400C for 7-10 minutes using hardwood charcoal reduces Na and Cl contents by 10-20% and contains large amounts of inorganic components as compared with the existing burned bay salt, thereby exhibiting relatively superior anti-cancer and anti-oxidizing effects. [Reference numerals] (S110) Filling a pottery with bay sa (S120) Heating a red clay kiln to a predetermined temperature by using hardwood charcoal; (S130) Placing the pottery containing the bay salt on the heated red clay kiln; (S140) Heating the red clay pottery for 7-10 minutes to cook the bay sa (S150) Taking out the red clay pottery containing the cooked bay salt from the red clay kiln
机译:本发明涉及一种通过燃烧月桂酸盐而制备能够去除有害物质并增加健康成分的月桂盐的方法。根据本发明的制备方法包括以下步骤:(a)用月桂盐填充红粘土陶器; (b)用硬木炭将红土窑加热到1000-1400℃; (c)将装有月桂盐的红土陶器放在加热的红土窑上; (d)将红土陶器放在窑上后,氧化月桂盐中所含的Na和Cl成分,然后在相同温度下加热红土陶器7-10分钟,从而燃烧月桂盐以补充盐分无机成分(e)在步骤(d)之后,从红土窑中取出包含烧过的月桂盐的红土陶器。因此,通过使用硬木木炭在1000-1400℃下加热7-10分钟而制备的月桂盐与现有的烧制月桂盐相比,将Na和Cl的含量降低了10-20%,并且含有大量的无机成分,从而显示出相对优异的品质。抗癌和抗氧化作用。 [附图标记](S110)用月桂盐填充陶器; (S120)通过使用硬木炭将红土窑加热至预定温度; (S130)将含有月桂盐的陶器放置在加热的红土窑上; (S140)加热红陶器7-10分钟以煮制月桂盐; (S150)从红土窑中取出含有煮熟的月桂盐的红土陶器

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号