Disclosed are a manufacturing method of artificial light-weight aggregates which have an uniformed foaming property of the inside of the aggregates, and artificial light-weight aggregates by using a material which comprises reject ash by controlling the inserting temperature, heating speed, sintering temperature, and having low specific gravity and absorptance without adding separate blowing agent, fusing agent. The present invention relates to a manufacturing method of artificial light-weight aggregates by using a material which comprises reject ash and temperature elevation sintering method which comprises: (a) a step of inserting a material to a preheated firing furnace; (b) a step of elevating the temperature of the furnace in which the material is inserted; (c) a step of maintaining in the optimum elevated temperature after finishing the elevation of the temperature; (d) discharging the material which is finished sintering after maintaining for a predetermined time. [Reference numerals] (AA) Embodiment 1-4; (BB) Embodiment 5-8; (CC) Embodiment 9-12; (DD) Comparison example 1-4
机译:公开了一种人造轻质骨料的制造方法,该方法在骨料内部具有均匀的起泡性能,并且通过使用包含杂质灰分的材料通过控制插入温度,加热速度,烧结温度来制造人造轻质骨料,比重和吸收率低,无需添加单独的发泡剂,定影剂。本发明涉及一种人造轻骨料的制造方法,该方法是使用一种包括废灰的材料和一种温度升高的烧结方法,该方法包括:(a)将材料插入预热的烧成炉中的步骤; (b)提高插入材料的炉子温度的步骤; (c)在温度升高完成后保持最佳高温的步骤; (d)在保持预定时间后排出完成烧结的材料。 [附图标记](AA)实施例1-4; (BB)实施例5-8; (CC)实施例9-12; (DD)比较例1-4

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号