The detached house or apartment and flats that the present invention relates to a kind of for preventing floor construction method noise use magnesia raw material and its curing agent, more specifically, it is related to the construction method for preventing floor noise, by making magnesia raw material, its curing agent slurries is mixed with the magnesium form of foam that micro bubble forms hardening to two layers of seat in upper part floor using driving method, provides soundproof effect. In construction method for preventing floor noise, the present invention includes: comprising steps of the quantity for providing bubble includes micro bubble and inorganic magnesia raw material and its inorganic hardener; Comprising steps of providing slurry, including an a large amount of micro bubbles; A kind of top placed step or construct slurry forms a large amount of three dimensional network structures and hardens when a large amount of microbubbles are included in hydration reaction to prevent floor noise on floor. Therefore, the present invention can play acoustic material, simultaneously as its high-intensitive sound insulating material passes through air layer between external impact sound building floor to reduce. ;The 2014 of copyright KIPO submissions;[Reference numerals] (AA) foaming agent dilution step; (BB) the step of bubble occurs; Magnesia raw material (CC) slurry; Curing agent (DD) dilution step; (EE) blending step; (FF) step is placed; (GG) curing schedule
机译:本发明涉及一种独立式住宅或公寓楼,用于防止地板噪声的方法使用氧化镁原料及其固化剂,更具体地,涉及一种通过使氧化镁为原料来防止地板噪声的构建方法。材料,其固化剂浆料与镁的泡沫形式混合,使用驱动方法将微气泡硬化成上部地板的两层座,提供隔音效果。在防止地板噪音的施工方法中,本发明包括:提供气泡的步骤包括:微气泡和无机氧化镁原料及其无机硬化剂。提供浆液的步骤,包括大量的微气泡;一种顶部放置的步骤或构造浆液会形成大量的三维网络结构,并且在水合反应中包含大量微气泡以防止地板上的噪音时会硬化。因此,本发明可以同时播放声学材料,因为其高强度的隔音材料穿过外部撞击声建筑地板之间的空气层以减少声学材料。 ; 2014年版权KIPO提交的文件; [参考数字](AA)发泡剂稀释步骤; (BB)发生气泡的步骤;镁原料(CC)浆;固化剂(DD)稀释步骤; (EE)混合步骤; (FF)步骤已放置; (GG)固化时间表

著录项

  • 公开/公告号KR20140046957A

    专利类型

  • 公开/公告日2014-04-21

    原文格式PDF

  • 申请/专利权人 PHILTEC CO. LTD.;I DONG HUI;

    申请/专利号KR20120113220

  • 发明设计人 NA PHIL CHAN;I DONG HUI;

    申请日2012-10-11

  • 分类号E04F15/20;E04F15/00;C04B16/04;C04B38/00;

  • 国家 KR

  • 入库时间 2022-08-21 15:43:12

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号