LITHIUM ION-CONDUCTIVE SOLID ELECTROLYTE, METHOD FOR PRODUCING SAME, SOLID ELECTROLYTE FOR LITHIUM SECONDARY BATTERY USING SUCH SOLID ELECTROLYTE, AND ALL-SOLID LITHIUM BATTERY USING SUCH SOLID ELECTROLYTE FOR SECONDARY BATTERY

机译:锂离子导电固体电解质,生产相同方法的锂,使用这种固体电解质的二次电池用固体电解质,以及使用这种固体二次电池的电解质的全固体锂电池

摘要

Disclosed is a lithium ion-conductive solid electrolyte exhibiting high lithium ion conductivity even at room temperature which is hardly oxidized and free from problems of toxicity and contains as components lithium (Li) element, boron (B) element, sulfur (S) element, and oxygen (O) element, and the ratio between sulfur element and oxygen element (O/S) is 0.01 to 1.43.
机译:公开了即使在室温下也显示高锂离子传导性的锂离子传导性固体电解质,其几乎不被氧化并且没有毒性问题,并且包含锂(Li)元素,硼(B)元素,硫(S)元素,和氧(O)元素,硫元素与氧元素的比率(O / S)为0.01至1.43。

著录项

  • 公开/公告号KR101354334B1

    专利类型

  • 公开/公告日2014-01-22

    原文格式PDF

  • 申请/专利权人

    申请/专利号KR20077015685

  • 申请日2006-01-10

  • 分类号H01M10/05;C03C3/064;H01B1/06;

  • 国家 KR

  • 入库时间 2022-08-21 15:41:41

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号