Eco-friendly warm-mix asphalt mixture and its manufacturing method

机译:环保型温拌沥青混合料及其制造方法

摘要

The present invention relates to an environment-friendly warm mix asphalt concrete mixture and a manufacture method thereof which comprises: a) a step of manufacturing an asphalt binder by mixing 85-96 weight% of dehydrated aspha 1.8-8 weight% of powdered styrene butadiene rubber (SBR); 1-12 weight% of polyethylene based oligomer; 0.2-1 weight% of sulfur; b) a step of heating the asphalt binder at 120-150C, and the aggregate at 120-150C respectively; c) a step of mixing the heated asphalt binder and the aggregate at 120-150C. [Reference numerals] (AA) A step of manufacturing an environment-friendly warm mix asphalt binder; (BB) A step of heating the asphalt binder at 120-150C, and the aggregate at 120-150C respectively; (CC) A step of mixing the heated asphalt binder and the aggregate at 120-150C.
机译:本发明涉及一种环保型温拌沥青混凝土混合料及其制造方法,包括:a)通过混合85-96重量%的脱水沥青来制备沥青结合料的步骤; 1.8-8重量%的粉状丁苯橡胶(SBR); 1-12重量%的聚乙烯基低聚物; 0.2-1重量%的硫; b)分别在120-150℃和120-150℃下加热沥青粘合剂的步骤; c)在120-150℃下混合加热的沥青粘合剂和骨料的步骤。 [附图标记](AA)制造环境友好的热拌沥青粘合剂的步骤; (BB)分别在120-150℃加热沥青结合料和在120-150℃加热骨料的步骤; (CC)在120-150℃下混合加热的沥青粘合剂和骨料的步骤。

著录项

  • 公开/公告号KR101365547B1

    专利类型

  • 公开/公告日2014-02-20

    原文格式PDF

  • 申请/专利权人

    申请/专利号KR20120074480

  • 发明设计人 손원익;

    申请日2012-07-09

  • 分类号C04B26/26;C04B24/26;C04B14/02;E01C7/18;

  • 国家 KR

  • 入库时间 2022-08-21 15:41:28

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号