A method for producing a polyester resin film includes melt extruding a polyester resin into a sheet shape, cooling and solidifying the polyester resin sheet on a casting drum, then longitudinally stretching the polyester resin sheet in the longitudinal direction, and then transversely stretching the longitudinally stretched polyester resin film in the transverse direction. The glass transition temperature of the polyester resin, Tg (° C.), the crystallinity of the film after the longitudinal stretching, Xc (%), the crystallization temperature of the film after the longitudinal stretching, Tc (° C.), film surface temperature at the entrance of the stretching zone of a transverse stretching apparatus 30, Ts (° C.), and film surface temperature at the exit of the stretching zone of the transverse stretching apparatus 30, Te (° C.), satisfy: 3≦̸Xc≦̸20; Tg−10≦̸Ts≦̸Tc+20; and Tc−10≦̸Te≦̸Tc+80.
机译:聚酯树脂膜的制造方法包括:将聚酯树脂熔融挤出成片状,在流延鼓上冷却并固化,然后在长度方向上纵向拉伸聚酯树脂片,然后在长度方向上横向拉伸。聚酯树脂薄膜在横向上。聚酯树脂的玻璃化转变温度Tg(℃),纵向拉伸后的膜的结晶度Xc(%),纵向拉伸后的膜的结晶温度,Tc(℃),膜横向拉伸装置30的拉伸区域的入口处的表面温度Ts(℃)和横向拉伸装置30的拉伸区域的出口处的膜表面温度Te(℃)满足: 3≦̸ Xc≦̸ 20; Tg&min ;; 10≦̸ Ts≦̸ Tc + 20;和Tc− 10≦̸ Te≦̸ Tc + 80。

著录项

  • 公开/公告号KR101416734B1

    专利类型

  • 公开/公告日2014-07-08

    原文格式PDF

  • 申请/专利权人

    申请/专利号KR20097019773

  • 申请日2008-03-25

  • 分类号B29C55/14;G02B1/11;G02B5/02;B29K67/00;

  • 国家 KR

  • 入库时间 2022-08-21 15:40:34

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号