首页> 外国专利> METHOD OF HYDROCRACKING, LOW B THE RATIO OF IMPROVED DISTILLATE AND IMPROVED OUTPUT OF OIL MATERIALS AND THEIR PROPERTIES

METHOD OF HYDROCRACKING, LOW B THE RATIO OF IMPROVED DISTILLATE AND IMPROVED OUTPUT OF OIL MATERIALS AND THEIR PROPERTIES

机译:加氢裂化的方法,低馏出物的馏出率和改善后的油料产量及其性质

摘要

1. A method for hydrocracking feedstock - vacuum gas oil, which is selective for the converted product a distillate boiling range of temperatures and gives output unconverted products suitable for use as a lubricant, the method comprising: providing raw material flow - vacuum gas oil having the nitrogen content is not greater than about 50 wt. ppm., and a sulfur content of no more than about 300 wt. ppm, the feed stream hydrocracking -. VGO step hydrocracking at high conversions stream of hydrogen-containing treat gas in the presence of a two-stage catalyst system at effective hydrocracking conditions sufficient to achieve the degree of conversion of over 55%, to form gidrokrekingaa product irazdelenie hydrocracking product converted product having a maximum of approximately 371 ° C (about 700 ° F) boiling point range, and unconverted product having and nterval boiling temperature with a minimum ratio of about 371 ° C (about 700 ° F), wherein the converted product has one or more cetane number of at least 45, the height of the smoke point of at least 20 mm and a sulfur content of not more than 12 wt. ppm., and unconverted product has one or more viscosity index of at least 80, a pour point of less than 5 ° C and a kinematic viscosity at about 100 ° C, of ​​at least 1 cSt, wherein a two-stage catalyst system comprises (1 ) USY catalyst comprising a Group VIII noble metal selected from platinum, palladium and with
机译:1.一种加氢裂化原料的方法-真空瓦斯油,其对转化产物在温度范围内的馏出物沸腾有选择性,并给出适合用作润滑剂的输出未转化产物,该方法包括:提供原料流-具有氮含量不大于约50重量%。 ppm,并且硫含量不超过约300wt。%。 ppm,进料流加氢裂化-。在两阶段催化剂体系的存在下,在足以实现超过55%转化率的有效加氢裂化条件下,在含氢处理气体的高转化率流下进行VGO步骤加氢裂化,以形成具有以下特征的gidrokrekingaa产物irazdelenie加氢裂化产物转化产物:最高沸点范围约为371°C(约700°F),未转化产物的沸点和沸点之间的最小比率约为371°C(约700°F),其中转化产物的十六烷值为一个或多个烟点的高度至少为45,烟点的高度至少为20 mm,硫含量不超过12 wt。 ppm。和未转化的产品,其一种或多种粘度指数至少为80,倾点小于5°C,运动粘度在约100°C下至少为1 cSt,其中两段催化剂该系统包括(1)USY催化剂,该催化剂包含选自铂,钯的VIII族贵金属,以及

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号