首页> 外国专利> METHOD OF PRODUCING POWDERS OF TITANIUM-, ZIRCONIUM- AND HAFNIUM-BASED ALLOYS DOPED WITH ELEMENTS NI, CU, TA, W, RE, OS, AND IR

METHOD OF PRODUCING POWDERS OF TITANIUM-, ZIRCONIUM- AND HAFNIUM-BASED ALLOYS DOPED WITH ELEMENTS NI, CU, TA, W, RE, OS, AND IR

机译:生产掺有元素Ni,Cu,TA,W,RE,OS和IR的钛,锆和HA基合金粉末的方法

摘要

FIELD: process engineering.;SUBSTANCE: invention relates to powder metallurgy. It can be used in production of pyrotechnic fuses, as gas absorbers in vacuum tubes, lamps, vacuum hardware and gas cleaners. Oxide of basic element selected from Ni, Zr and Hf is mixed with alloying metal powder selected from Ni, Cu, Ta, W, Re, Os or Ir and with reducing agent powder. Produced mix is heated in kiln in atmosphere of argon to initiation of reduction reaction. Reaction product is leached, flushed and dried. Said oxide of basic element features mean particle size of 0.5-20 mcm, BET specific surface of 0.5-20 m2/g and minimum content of said oxide of 94 wt %.;EFFECT: powder with reproducible combustion time, specific surface and distribution of articles in sizes and time.;23 cl, 5 ex
机译:粉末冶金技术领域本发明涉及粉末冶金。它可用于生产烟火保险丝,用作真空管,灯,真空硬件和气体清洁器中的气体吸收剂。将选自Ni,Zr和Hf的碱性元素的氧化物与选自Ni,Cu,Ta,W,Re,Os或Ir的合金金属粉末和还原剂粉末混合。产生的混合物在氩气气氛下在窑中加热以引发还原反应。将反应产物浸出,冲洗并干燥。所述基本元素的氧化物的特征在于平均粒度为0.5-20mcm,BET比表面积为0.5-20m 2 / g,并且所述氧化物的最小含量为94wt%。效果:具有可再现性的粉末燃烧时间,比表面积和物品在尺寸和时间上的分布;; 23 cl,5 ex

著录项

  • 公开/公告号RU2507034C9

    专利类型

  • 公开/公告日2014-08-10

    原文格式PDF

  • 申请/专利权人 SHEMETALL GMBKH;

    申请/专利号RU20100139561

  • 申请日2009-02-27

  • 分类号B22F9/20;C22C1/04;C22C14;

  • 国家 RU