PROBLEM TO BE SOLVED: To provide a method of preparing high strength concrete capable of resolving problems of 1) and 2) at same time, where a) viscosity of concrete during preparation is high and flowability with time after preparation dramatically reduces (viscosity of concrete becomes high with time) and 2) enhancement of long term strength (compressive strength at 91 days of material age) of a resulting cured body is reduced when concrete is subject to a thermal history with temperature increase by heat generation during a process of curing by a hydration reaction, a high strength concrete obtained by the preparation method, a cured body obtained by curing the high strength concrete.;SOLUTION: There is provided a method of preparing high strength concrete by using low heat generating Portland cement, water, a fine aggregate, a coarse aggregate and following multifunctional admixture with percentage of 0.1 to 1.5 pts.mass of a specific multifunctional admixture containing a specific 3 components at a specific ratio per 100 pts.mass of the low heat generating Portland percentage.;COPYRIGHT: (C)2015,JPO&INPIT
机译:要解决的问题:提供一种能够同时解决1)和2)问题的高强度混凝土的制备方法,其中a)在制备过程中混凝土的粘度很高,并且制备后随时间的流动性会大大降低(混凝土的粘度)随时间而变高); 2)当混凝土经历热过程,并且随着在固化过程中热量的产生而温度升高,则所得固化体的长期强度(在材料寿命的91天时的抗压强度)的提高会降低。水合反应,通过该制备方法获得的高强度混凝土,通过固化该高强度混凝土获得的固化体。;解决方案:提供了一种使用低热量生成的硅酸盐水泥,水,细粉制备高强度混凝土的方法。骨料,粗骨料和随后的多功能混合物,其质量百分比为0.1至1.5 pts。每100 pts质量的3种成分按低热量产生的波特兰百分率质量计算;版权:(C)2015,JPO&INPIT

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号