PROBLEM TO BE SOLVED: To provide a high strength cement mortar composition having high compression strength without needs for large scale and special manufacturing facility.SOLUTION: There is provided a high strength concrete composition containing cement, inorganic fine powder, water, a fine aggregate, a coarse aggregate, a water-reducing agent, an antifoam agent and metal fine particles, the cement contains 10.0 mass% to 70.0 mass% of CS and 10.0 mass% to 70.0 mass% of CS, the fine aggregate contains ferronickel slag. Also there is provided a manufacturing method of a high strength concrete cured body including a pre-curing process for conducting curing in air at 15 to 25°C for 1 day to 5 days, a primary curing process for conducting curing in water at 20 to 60°C for 1 day to 7 days and a second curing process for conducting curing in water or air at 80 to 200°C for 1 day to 21 days.SELECTED DRAWING: None
机译:要解决的问题:提供不需要高规模和特殊制造设施的,具有高抗压强度的高强度水泥砂浆组合物。解决方案:提供一种包含水泥,无机细粉,水,细骨料,粗骨料,减水剂,消泡剂和金属微粒。水泥中含有10.0质量%〜70.0质量%的CS和10.0质量%〜70.0质量%的CS,细骨料含有镍铁渣。还提供了一种高强度混凝土固化体的制造方法,该方法包括用于在15至25°C的空气中进行1天至5天的固化的预固化过程,以及用于在20至20°C的水中进行固化的初级固化过程。 60°C持续1天至7天,然后进行第二次固化工艺,以在80至200°C的水或空气中进行1天至21天的固化。

著录项

  • 公开/公告号JP2016098141A

    专利类型

  • 公开/公告日2016-05-30

    原文格式PDF

  • 申请/专利权人 UBE IND LTD;

    申请/专利号JP20140236068

  • 发明设计人 KIRIYAMA HIROKAZU;SATO YOSHIHIDE;

    申请日2014-11-21

  • 分类号C04B28/02;C04B14/48;C04B18/14;C04B22/06;C04B24/26;C04B24/32;C04B40/02;

  • 国家 JP

  • 入库时间 2022-08-21 14:45:58

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号