PROBLEM TO BE SOLVED: To provide a phenol resin binder composition capable of increasing hardening speed.;SOLUTION: A binder composition forms a binder layer on a surface of a refractory aggregate in a binder coated refractory formed by coating the binder layer on the surface of the refractory aggregate. A principal component of a binder is phenol resin, and trihydric phenol is contained by 1 to 60 mass% in the phenol resin, which is the principal component of the binder. By the trihydric phenol being contained in the phenol resin, time required for the phenol resin to turn into gel is shortened, it is possible to further increase hardening speed.;COPYRIGHT: (C)2015,JPO&INPIT
机译:解决的问题:提供一种能够提高固化速度的酚醛树脂粘合剂组合物;解决方案:粘合剂组合物在耐火骨料的表面上形成粘合剂层,该耐火骨料通过在粘合剂表面上涂覆粘合剂层而形成。耐火骨料。粘合剂的主要成分是酚醛树脂,酚醛树脂中作为粘合剂的主要成分的三元酚的含量为1〜60质量%。通过在酚醛树脂中包含三元酚,可以缩短酚醛树脂变成凝胶所需的时间,并可以进一步提高固化速度。;版权所有:(C)2015,JPO&INPIT

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号