CLINKER PRODUCTION METHOD AND APPARATUS WHOSE FREE LIME CONTENT CONTROLLED BASED ON QUARTZ CRYSTALLITE DIAMETER

机译:基于石英晶体直径的游离石灰含量控制的熟料生产方法和装置

摘要

PROBLEM TO BE SOLVED: To provide a clinker production method in which the control of clinker free lime content is easy.;SOLUTION: Provided is a clinker production method in which the free lime content in a clinker is controlled by adjusting the input amount of a mineralizer based on the quartzite quartz crystallite diameter, and in which the free lime content is controlled by inputting a mineralizer by 0.12 to 0.14 kg/t-cli as fluorine amount for every time the quartz crystallite diameter increases by 50 nm for the case when the clinker free lime content increases by 0.1 to 0.3 wt.% for every time the quartz crystallite diameter increases by 50 nm when in no mineralizer addition, and by calcinating the same.;COPYRIGHT: (C)2015,JPO&INPIT
机译:解决的问题:提供一种易于控制熟料中游离石灰含量的熟料生产方法。解决方案:提供了一种熟料生产方法,其中通过调整水泥熟料的输入量来控制熟料中游离石灰的含量。矿化剂基于石英岩石英微晶直径,并且每当石英微晶直径增加50 nm时,通过将矿化剂的氟含量输入为0.12-0.14 kg / t-cli,来控制游离石灰含量。不添加矿化剂并对其进行煅烧时,石英微晶直径每增加50 nm,熟料中游离石灰的含量就会增加0.1至0.3 wt。%。版权所有:(C)2015,JPO&INPIT

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号