Blast furnace operation method using ferro-coke

机译:使用铁焦的高炉操作方法

摘要

The amount of a carbon iron composite used is appropriately adjusted when the carbon iron composite is used in a blast furnace, whereby a stable operation is provided. Ore and coke including the carbon iron composite and conventional coke are charged into the blast furnace. The percentage of the carbon iron composite used is 2% to 50% by mass of the coke. The percentage of the carbon iron composite used is preferably 25% by mass or more. The carbon iron composite preferably has a particle size of 15 mm to 40 mm. The carbon iron composite preferably has an iron content of 10% to 40% by mass.
机译:当在高炉中使用碳铁复合物时,可以适当地调节碳铁复合物的使用量,从而提供稳定的操作。将包括碳铁复合物和常规焦炭的矿石和焦炭装入高炉。所使用的碳铁复合物的百分比为焦炭的2质量%至50质量%。碳铁复合材料的使用比例优选为25质量%以上。碳铁复合材料的粒径优选为15mm至40mm。碳铁复合材料优选具有10质量%至40质量%的铁含量。