首页> 外国专利> METHOD OF PREPARING IRON CARBIDE/CARBON NANOCOMPOSITE CATALYST CONTAINING POTASSIUM FOR HIGH TEMPERATURE FISCHER-TROPSCH SYNTHESIS REACTION AND THE IRON CARBIDE/CARBON NANOCOMPOSITE CATALYST PREPARED THEREBY, AND METHOD OF MANUFACTURING LIQUID HYDROCARBON USING THE SAME AND LIQUID HYDROCARBON MANUFACTURED THEREBY

METHOD OF PREPARING IRON CARBIDE/CARBON NANOCOMPOSITE CATALYST CONTAINING POTASSIUM FOR HIGH TEMPERATURE FISCHER-TROPSCH SYNTHESIS REACTION AND THE IRON CARBIDE/CARBON NANOCOMPOSITE CATALYST PREPARED THEREBY, AND METHOD OF MANUFACTURING LIQUID HYDROCARBON USING THE SAME AND LIQUID HYDROCARBON MANUFACTURED THEREBY

机译:包含钾的碳化铁/碳纳米复合催化剂的制备方法,用于高温费-托合成反应和制备的碳化铁/碳纳米复合催化剂,以及制备液态烃和制备液态烃的方法

摘要

This invention relates to a method of preparing an iron carbide/carbon nanocomposite catalyst containing potassium for high temperature Fischer-Tropsch (FT) synthesis reaction and the iron carbide/carbon nanocomposite catalyst prepared thereby, and a method of manufacturing a liquid hydrocarbon using the same and a liquid hydrocarbon manufactured thereby, wherein a porous carbon support is uniformly impregnated with an iron hydrate using melt infiltration, and potassium is also supported together via various addition processes, including a pre-addition process of a potassium salt which is ground upon impregnation with the iron hydrate, or a mid- or post-addition process of a potassium solution using incipient wetness impregnation after impregnation with the iron hydrate. Accordingly, the highly active iron carbide/potassium/carbon composite catalyst for high temperature FT reaction in which 5˜30 wt % of active iron carbide particles are supported on the porous carbon support can be obtained and is structurally stable to heat even in high temperature FT reaction of 300° C. or more, and liquid hydrocarbons can be selectively obtained at high yields.
机译:本发明涉及制备用于高温费-托(FT)合成反应的含有钾的碳化铁/碳纳米复合催化剂的方法和由此制备的碳化铁/碳纳米复合催化剂,以及使用该催化剂制备液态烃的方法以及由此制得的液态烃,其中多孔碳载体通过熔融渗透用水合铁均匀地浸渍,并且钾也通过各种添加过程一起负载在一起,包括钾盐的预添加过程,所述钾盐在浸渍时被研磨。水合铁,或在水合铁浸渍后使用初期湿润浸渍的钾溶液的中间添加过程或后添加过程。因此,可以获得将5〜30重量%的活性碳化铁颗粒负载在多孔碳载体上的用于高温FT反应的高活性碳化铁/钾/碳复合催化剂,并且即使在高温下也对热稳定。 300℃以上的FT反应,可以高收率选择性地得到液态烃。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号