首页> 外国专利> MICROGEL CONTAINING TREAD MIXTURE FOR WINTER TYRES

MICROGEL CONTAINING TREAD MIXTURE FOR WINTER TYRES

机译:含微胎的冬季胎混合物

摘要

(L SBR)(BR)(NR)The present invention relates to vulcanisable rubber mixtures containing at least the following components: I) 100 pbw of an oil free rubber matrix consisting of a) 15 79 pbw preferably 20 70 pbw of at least one solution SBR (L SBR) (oil free) with a glass transition temperature (Tg) between 70°C and 10°C b) 20 75 pbw preferably 25 70 pbw of at least one 1 4 cis polybutadiene (BR) (oil free) with a glass transition temperature (Tg) between 95°C and 115°C c) 1 37.5 pbw preferably 5 35 pbw of natural rubber (NR) (oil free) and/or at least one synthetically produced polyisoprene (IR) with a glass transition temperature (Tg) between 50°C and 75°C relative to the oil free natural rubber (NR) or the oil free synthetically produced polyisoprene (IR); II) at least one polybutadiene based microgel that contains hydroxyl groups; III) at least one oxide filler that contains hydroxyl groups; IV) at least one polysulphide containing alkoxysilane; V) at least one vulcanisation agent; VI) optionally at least one rubber additive.
机译:(L SBR)(BR)(NR)本发明涉及至少包含以下组分的可硫化橡胶混合物:I)100 pbw的无油橡胶基质,其由a)15 79 pbw,优选20 70 pbw的至少一种组成溶液SBR(L SBR)(无油),玻璃化温度(Tg)在70°C和10°C之间b)20 75 pbw,优选25 70 pbw的至少一种1 4顺式聚丁二烯(BR)(无油)玻璃化转变温度(Tg)在95°C至115°C之间c)1 37.5 pbw,优选5 35 pbw的天然橡胶(NR)(无油)和/或至少一种合成的聚异戊二烯(IR)与玻璃相对于无油天然橡胶(NR)或无油合成生产的聚异戊二烯(IR)的转变温度(Tg)在50°C至75°C之间; II)至少一种含羟基的聚丁二烯基微凝胶; III)至少一种含有羟基的氧化物填料; IV)至少一种含有烷氧基硅烷的多硫化物; V)至少一种硫化剂; VI)任选地至少一种橡胶添加剂。

著录项

  • 公开/公告号IN6609DEN2014A

    专利类型

  • 公开/公告日2015-05-22

    原文格式PDF

  • 申请/专利权人 LANXESS DEUTSCHLAND GMBH;

    申请/专利号IN2014DELNP6609

  • 发明设计人 OBRECHT WERNER;STEGER LOTHAR;

    申请日2014-08-06

  • 分类号C08L19;C08K5/548;C08L7;

  • 国家 IN

  • 入库时间 2022-08-21 15:14:06

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号