The invention relates to a method for producing monolithic titanium suboxide TiOx ceramic electrode for water electrochemical treatment and to an electrode produced using this method. The method for producing an electrode is performed in the following way: from the mixture of titanium oxide TiO2 powder, water and binder, a green body in the shape of a flat strip is formed by extrusion, a green body is dried, a hole (2) for fastening an electroconductive element (4) in one end of the dried green body is made, a monolithic titanium suboxide TiOx, where x is in the range from 1.95 to 1.97, ceramic strip (1) with the open porosity 10-30% is formed by thermal treating of the green body, on the surface of the flat strip around the hole (2) at least 5 mm wide zone of 5-20 microns thick electroconductive coating (3) is sputtered, creating continuous metal-ceramic connection, through the hole (2) with a screw (6), a spring washer (7) and a nut (8) the electroconductive element (4) to which an electrical wire (5) is connected, is motionlessly mechanically fastened to the monolithic titanium suboxide ceramic strip (1) where electroconductive coating is, thereafter, using vacuum impregnation, the end of the electrode (9) where electric connection is created, is sealed with the epoxide resin, sealing it off completely. The produced electrode has large specific active surface and its operating duration in the water electrochemical treatment devices with the current density 5-10 mA/cm2 exceeds 2 years.
机译:本发明涉及用于水电化学处理的整体式低氧化钛TiO x陶瓷电极的制造方法,以及使用该方法制造的电极。电极的制造方法如下进行:从氧化钛TiO 2粉末,水和粘合剂的混合物中挤出形成扁平带状的生坯,将生坯干燥后,开孔( 2)制造用于将导电元件(4)固定在干燥的生坯的一端中的整体式低氧化钛TiO x,其中x在1.95至1.97的范围内,陶瓷条(1)的孔隙率为10-30通过生坯的热处理形成%,在孔(2)周围的扁平条的表面上溅射至少5 mm宽的5-20微米厚的导电涂层(3),形成连续的金属-陶瓷连接通过带有螺钉(6),弹簧垫圈(7)和螺母(8)的孔(2),将连接有电线(5)的导电元件(4)机械固定地固定在整体结构上此后使用真空吸尘的低氧化钛陶瓷条(1)在浸渍过程中,将形成电连接的电极(9)的一端用环氧树脂密封,将其完全密封。所制得的电极具有较大的比活性表面,并且在水电化学处理装置中其电流密度为5-10mA / cm 2的工作持续时间超过2年。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号