METHOD FOR WELDING TWO EDGES OF ONE OR MORE STEEL PARTS TO EACH OTHER INCLUDING A HEAT TREATMENT STEP AFTER THE WELDING STEP: PENSTOCK OBTAINED WITH SUCH A METHOD

机译:在焊接步骤后将一个或多个钢制零件的两个边缘焊接在一起的方法,包括热处理步骤:采用这种方法获得的喷枪

摘要

The present application describes a method for welding two parts to each other. The two parts are made from steel having a high thermomechanical yield strength. The welding method includes a welding step in which a weld bead is created inducing a heat-affected zone to appear. The method also includes a heat treatment step having a heating step, during which at least one portion of the weld bead and the HAZ is gradually heated to a treatment temperature; then a holding step in which the portion of the weld bead and the HAZ is kept at the treatment temperature; then a cooling step in which the HAZ and the weld bead are gradually cooled and pass from the austenitic transformation end temperature to the martensitic transformation end temperature of the steel of the parts in a time between 7.5 s and 8.5 s, and pass from the austenitic transformation end temperature to the martensitic transformation end temperature in a time shorter than 15.5 s. The present application also describes a penstock obtained with such a method.
机译:本申请描述了一种用于将两个部件彼此焊接的方法。这两个部分由具有高热机械屈服强度的钢制成。焊接方法包括焊接步骤,其中形成焊缝,引起热影响区出现。该方法还包括具有加热步骤的热处理步骤,在该加热步骤中,将焊缝和HAZ的至少一部分逐渐加热至处理温度;然后进行保持步骤,其中将焊缝和HAZ的一部分保持在处理温度下;然后进行冷却步骤,在此步骤中,在7.5 s和8.5 s之间的时间内,将HAZ和焊缝逐渐冷却,并从奥氏体转变结束温度达到零件钢的马氏体转变结束温度,然后从奥氏体转变为转变结束温度到马氏体转变结束温度的时间少于15.5 s。本申请还描述了用这种方法获得的压力笔。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号